Major Maciej, Adamczyk Izabela, Kalinowski Jarosław
Faculty of Civil Engineering, Czestochowa University of Technology, Dabrowskiego 69, 42-201 Częstochowa, Poland.
Materials (Basel). 2023 Jul 16;16(14):5028. doi: 10.3390/ma16145028.
This paper discusses an innovative APS hollow block wall with a frame made of concrete modified with recycled materials. The technical data of the hollow block, the percentages of the recycled materials, including SBR rubber granules and PET flakes in the modified concrete, and the composition of the concrete modified with this mixture of recycled additives, are presented. To demonstrate the effectiveness of the solution in reducing mechanical vibrations, the effect of the interaction of different frequencies of the mechanical wave on reducing these vibrations was evaluated for APS blocks and Alpha comparison blocks. The test was carried out on a developed test stand dedicated to dynamic measurements for sixteen frequencies in the range from 8 to 5000 Hz, forcing a sinusoidal course of vibrations. The results are presented graphically and show that the new type of APS hollow block wall was much more effective in reducing mechanical vibrations. This efficiency was in the range from 10 to 51% for 12 out of the tested 16 frequencies. For the frequencies of 8, 16, 128, and 2000 Hz, the values were obtained with a difference of 3.58% in favor of the APS hollow block. In addition, the study of the damping effectiveness of the APS hollow blocks, in relation to the vibrations generated by an M-400 impact mill, showed that the APS block wall had a higher damping efficiency of 16.87% compared to the Alpha hollow block for the signal reading on the floor next to the mill, and 18.68% for the signal reading on the mill body. The modified concrete used in the production of the APS hollow blocks enabled the effective use of two recycled materials, SBR rubber and polyethylene terephthalate, in the form of PET flakes.
本文讨论了一种创新的APS空心砌块墙,其框架由用回收材料改性的混凝土制成。文中给出了空心砌块的技术数据、回收材料的百分比,包括改性混凝土中的丁苯橡胶颗粒和聚对苯二甲酸乙二酯片,以及用这种回收添加剂混合物改性的混凝土的成分。为了证明该解决方案在降低机械振动方面的有效性,评估了机械波不同频率的相互作用对APS砌块和Alpha对比砌块减少这些振动的影响。该测试在一个专门用于动态测量的试验台上进行,该试验台针对8至5000Hz范围内的16个频率,施加正弦振动过程。结果以图形方式呈现,表明新型APS空心砌块墙在减少机械振动方面更有效。在测试的16个频率中的12个频率下,这种效率在10%至51%的范围内。对于8Hz、16Hz、128Hz和2000Hz的频率,获得的值有利于APS空心砌块,相差3.58%。此外,关于APS空心砌块相对于M - 400冲击磨产生的振动的阻尼有效性的研究表明,与Alpha空心砌块相比,APS砌块墙在磨机旁边地板上的信号读数的阻尼效率更高,为16.87%,在磨机主体上的信号读数的阻尼效率为18.68%。用于生产APS空心砌块的改性混凝土能够有效地使用两种回收材料,即丁苯橡胶和聚对苯二甲酸乙二酯形式的PET片。