Rk Radhi, Hegde Divya, Mc Juraise, Ummer Haseena, Nazer Nadeem, Mk Jyothsna
Prosthodontics, MES Dental College, Perinthalmanna, IND.
Prosthodontics, Bangalore Institute of Dental Sciences, Bangalore, IND.
Cureus. 2023 Aug 30;15(8):e44389. doi: 10.7759/cureus.44389. eCollection 2023 Aug.
One of the greatest benefits of contemporary restorative dentistry is the creation of fixed partial dentures. The retention and durability of the fixed partial dentures may be improved by using a variety of tooth preparation methods, surface treatments, and luting resins.
To measure the shear binding strength of resin cement to saliva-contaminated lithium disilicate (LDS) ceramic after being exposed to various cleaning treatments.
Over 30 LDS samples were examined. In Group 1, a cleansing solution comprising 15% zirconium oxide (Ivoclean) was employed for a duration of 20 s. This was succeeded by a rinsing phase lasting 15 s utilizing deionized water, followed by a 15-s period for drying. Subsequently, a final stage of air drying was conducted over a span of 15 s. In contrast, Group 2 underwent a washing procedure of 20 s involving a cleansing solution containing 30% sodium silicate. This was then ensued by a rinsing interval of 15 s with deionized water, succeeded by an air-drying process spanning 15 s. After applying cleaning solutions to the surface and adhering the specimens to the composite blocks using resin cement Multilink Automix (Ivoclar Vivadent, Schaan, Liechtenstein), the shear bond strength was assessed.
Using a 30% sodium silicate solution (Group 2), we were able to get the highest mean shear bond strength value after saliva-contaminated LDS. Group 1, 15% zirconium oxide (Ivoclean) had the weakest decontamination agents as measured by mean shear bond strengths. The shear bond strength values of the two groups were found to vary significantly between individuals using the independent sample -test. LDs ceramic cleaned with a 30% sodium silicate solution had a higher shear bond strength than ceramic cleaned with Ivoclean (p<0.05).
The application of a 30% sodium silicate solution rendered the highest shear bond strength for saliva-contaminated LDS ceramic. In comparison, ceramic cleaned with Ivoclean exhibited notably lower shear bond strength values. The outcome of this investigation highlights the potential of diverse cleaning agents in influencing the adhesive qualities of resin cement, thereby contributing to the enhancement of fixed partial denture durability and efficacy.
当代修复牙科的最大益处之一是固定局部义齿的制作。通过使用各种牙体预备方法、表面处理和粘结树脂,可以提高固定局部义齿的固位力和耐久性。
测量经各种清洁处理后,树脂水门汀与受唾液污染的二硅酸锂(LDS)陶瓷之间的剪切粘结强度。
检查了30多个LDS样本。在第1组中,使用含15%氧化锆的清洁溶液(Ivoclean)20秒。随后用去离子水冲洗15秒,接着干燥15秒。随后进行15秒的最终空气干燥阶段。相比之下,第2组进行了20秒的清洗程序,使用含30%硅酸钠的清洁溶液。然后用去离子水冲洗15秒,接着进行15秒的空气干燥过程。在将清洁溶液应用于表面并用树脂水门汀Multilink Automix(义获嘉伟瓦登特,沙恩,列支敦士登)将标本粘结到复合块上后,评估剪切粘结强度。
使用30%硅酸钠溶液(第2组),在受唾液污染的LDS之后,我们能够获得最高的平均剪切粘结强度值。通过平均剪切粘结强度测量,第1组含15%氧化锆(Ivoclean)的去污剂最弱。使用独立样本检验发现,两组的剪切粘结强度值在个体之间有显著差异。用30%硅酸钠溶液清洁的LDS陶瓷比用Ivoclean清洁的陶瓷具有更高的剪切粘结强度(p<0.05)。
30%硅酸钠溶液的应用使受唾液污染的LDS陶瓷具有最高的剪切粘结强度。相比之下,用Ivoclean清洁的陶瓷表现出明显较低的剪切粘结强度值。这项研究的结果突出了不同清洁剂在影响树脂水门汀粘结质量方面的潜力,从而有助于提高固定局部义齿的耐久性和功效。