Kord Zeinab, Taheri Ali, Ghaffari Mostafa, Sharifian Salim
Fish Processing Technology Division, Faculty of Marine Sciences, Chabahar Maritime University, Chabahar 99717-78631, Iran.
Foods. 2024 Feb 9;13(4):538. doi: 10.3390/foods13040538.
Scale gelatin films derived from croaker fish and infused with () extract (PE) at concentrations of 0.3% and 0.7% were produced. A control film, void of extract, was employed for comparative purposes. The thickness of each film was found to be statistically insignificant ( > 0.05). The results show that the highest solubility (78.57 ± 3.57%) was found for the glycerol film, and the least permeability was found for the water vapor (0.74 ± 0.09 ×10g smPa); however, the water vapor permeability (WVP) and water solubility (WS) of the films that contained PE were considerably lower than those of the control film ( < 0.05). In contrast to the control film, those infused with 0.7% PE exhibited exceptional UV-barrier properties (>99%) and favorable thermal characteristics. The highest and lowest antioxidant activities were found for the 7% extract (56.96 ± 2.6%) and the glycerol film (40.66 ± 2.46%), respectively. No antibacterial activity was observed in these films. Microscopic pictures showed that all three films had a uniform and plain surface. Fourier transform infrared spectroscopy-attenuated total reflectance (FTIR-ATR) analysis revealed distinct amide bands and protein-polyphenol interactions within the films that contained the extract.
制备了源自黄花鱼的明胶膜,并分别注入浓度为0.3%和0.7%的()提取物(PE)。制备了不含提取物的对照膜用于比较。发现各膜的厚度在统计学上无显著差异(>0.05)。结果表明,甘油膜的溶解度最高(78.57±3.57%),水蒸气渗透率最低(0.74±0.09×10g smPa);然而,含PE的膜的水蒸气透过率(WVP)和水溶性(WS)显著低于对照膜(<0.05)。与对照膜相比,注入0.7%PE的膜表现出优异的紫外线阻隔性能(>99%)和良好的热性能。7%提取物膜(56.96±2.6%)和甘油膜(40.66±2.46%)的抗氧化活性分别最高和最低。这些膜未观察到抗菌活性。显微镜照片显示,所有三种膜的表面均均匀平整。傅里叶变换红外光谱-衰减全反射(FTIR-ATR)分析揭示了含提取物的膜内有明显的酰胺带和蛋白质-多酚相互作用。