Moberg L E
Acta Odontol Scand. 1985 Aug;43(4):215-22. doi: 10.3109/00016358509046501.
Specimens of various types of dental casting alloys were stored in phosphate-buffered 0.9% NaCl solution for 35 weeks. Every 7 weeks the solutions were changed and analyzed with regard to elements released from the alloys. The release of Cu from type III gold alloy increased in contact with gold alloys for metallo-ceramic use in a 1:2 area relation. However, when the area relation was reversed, no difference in the amounts of elements released was observed. Crevice corrosion was initiated with one of the Co-Cr alloys in contact with type III gold alloy. The crevice corrosion increased the amounts of Co and Cr released into the solutions. The release of Ni and Cr from the Ni-Cr alloys was prominent. These alloys were very susceptible to crevice corrosion. With one of the Ni-Cr alloys the release of elements increased in contact with type III gold alloy.
将各种类型的牙科铸造合金样本储存在磷酸盐缓冲的0.9%氯化钠溶液中35周。每7周更换一次溶液,并分析合金释放的元素。III型金合金中铜的释放量在与用于金属陶瓷的金合金以1:2的面积关系接触时增加。然而,当面积关系颠倒时,未观察到释放元素量的差异。缝隙腐蚀是由一种钴铬合金与III型金合金接触引发的。缝隙腐蚀增加了释放到溶液中的钴和铬的量。镍铬合金中镍和铬的释放很显著。这些合金极易发生缝隙腐蚀。对于其中一种镍铬合金,与III型金合金接触时元素释放量增加。