Suppr超能文献

黄蓍胶和水葫芦纤维素接枝聚(乙烯基磺酸-co-丙烯酰胺)复合材料的合成、表征及柱吸附性能。

Synthesis, characterization and column adsorption properties of gum ghatti and water hyacianth derived cellulose grafted poly(vinyl sulfonic acid-co-acrylamide) composites.

机构信息

Department of Polymer Science and Technology, University of Calcutta, 92 A.P.C. Road, Kolkata 700009, West Bengal, India.

Department of Polymer Science and Technology, University of Calcutta, 92 A.P.C. Road, Kolkata 700009, West Bengal, India.

出版信息

Int J Biol Macromol. 2024 May;268(Pt 1):131652. doi: 10.1016/j.ijbiomac.2024.131652. Epub 2024 Apr 20.

Abstract

Vinylsulfonic acid (VSA), acrylamide (AM) and N, N methylene bis acrylamide(MBA) were copolymerized by radical polymerization in the presence of gum ghatti (GG) and treated water hyacianth (WH) in water. Several composite copolymers were prepared by varying the i) AM: VSA molar ratios ii) wt% of GG and iii) wt% of treated WH based on a Box-Behnken Design(BBD) of a response surface methodology (RSM) model with three input variables and the batch adsorption capacity (mg/g) of 100 mg/L Cd (II) from water as response. The composite polymer was characterized by Fourier transform Infrared spectroscopy (FTIR), X-ray diffraction (XRD), thermogravimetric analysis(TGA), X- ray photo electron spectroscopy (XPS), compressive strength, pH reversibility, pH at point zero charge (pH), Brunauer-Emmett-Teller (BET) surface area and scanning electron microscopy (SEM). The network parameters of the composites were determined. The copolymer composite prepared with AM: VSA of 5:1 containing 10 wt% GG and 4 wt% treated WH showed an optimum batch adsorption capacity of 399.15 mg/g Cd (II) from water containing 100 mg/L Cd (II). The same composite showed an adsorption capacity of 170.1 mg/g and a removal% of 31.5 at a feed concentration/feed flow rate/bed height of 150 mgL/30mLmin/30 mm in a fixed bed column.

摘要

在水中,采用自由基聚合的方法,使 vinylsulfonic 酸(VSA)、丙烯酰胺(AM)和 N, N 亚甲基双丙烯酰胺(MBA)与 Gum ghatti(GG)和处理过的水葫芦(WH)共聚。根据响应面法(RSM)模型的 Box-Behnken 设计(BBD),通过改变 i)AM:VSA 摩尔比 ii)GG 的重量百分比和 iii)处理过的 WH 的重量百分比,制备了几种复合共聚物,其中三个输入变量是基于 100mg/L Cd(II)在水中的批吸附容量(mg/g)作为响应。复合聚合物通过傅里叶变换红外光谱(FTIR)、X 射线衍射(XRD)、热重分析(TGA)、X 射线光电子能谱(XPS)、抗压强度、pH 可逆性、零电荷 pH(pH)、Brunauer-Emmett-Teller(BET)表面积和扫描电子显微镜(SEM)进行了表征。测定了复合材料的网络参数。由 AM:VSA 为 5:1 组成、含有 10wt% GG 和 4wt%处理过的 WH 的共聚物复合材料在含有 100mg/L Cd(II)的水中显示出最佳的 399.15mg/g Cd(II)的批吸附容量。在固定床柱中,当进料浓度/进料流速/床高为 150mgL/30mLmin/30mm 时,相同的复合材料的吸附容量为 170.1mg/g,去除率为 31.5%。