Performance of High-Dose Reclaimed Asphalt Mixtures (RAPs) in Hot In-Place Recycling Based on Balanced Design.

作者信息

Jiang Lei, Shen Junan, Wang Wei

机构信息

Jiangsu Technology Industrialization and Research Center of Ecological Road Engineering, Suzhou University of Science and Technology, Suzhou 215011, China.

Department of Civil Engineering and Construction, Georgia Southern University, Statesboro, GA 30458, USA.

出版信息

Materials (Basel). 2024 Apr 29;17(9):2096. doi: 10.3390/ma17092096.

Abstract

This study endeavors to employ a balanced design methodology, aiming to equilibrate the resistance to rutting and cracking exhibited by hot in-place recycling asphalt mixtures containing a high dose of reclaimed asphalt pavement (RAP). The primary goal is to ascertain the optimal amount of new binder necessary for practical engineering applications, ensuring a balanced rutting and crack resistance performance of recycled asphalt mixtures. The investigation mainly employed wheel-tracking tests and semi-circular bending tests to assess the rutting and cracking performance of recycled asphalt mixtures with a different dose of RAP (in China, it is common to use RAP with 80% and 90% content as additives for preparing hot in-place recycling asphalt mixtures), and varying quantities of new binders (10%, 20%, and 30% of the binder content in the total RAP added). The results indicated that the addition of new binder reduced the resistance to rutting of the recycling asphalt mixtures but improved their resistance to cracking. Furthermore, for the recycling asphalt mixture with 80% RAP content aged for 5 days, the optimal new binder content is 1.52%, while the mixture with 90% RAP content requires 1.23% of new binder. After 10 days of aging, the optimal new binder content for the recycling asphalt mixture with 80% RAP content is 1.55%, while the mixture with 90% RAP content requires 1.28% of new binder.

摘要

本研究致力于采用一种平衡设计方法,旨在平衡高剂量再生沥青路面(RAP)的热就地再生沥青混合料所表现出的抗车辙和抗裂性能。主要目标是确定实际工程应用所需的最佳新粘结剂用量,确保再生沥青混合料具有平衡的抗车辙和抗裂性能。该研究主要采用车辙试验和半圆弯曲试验来评估不同剂量RAP(在中国,通常使用80%和90%含量的RAP作为添加剂来制备热就地再生沥青混合料)以及不同数量新粘结剂(占总RAP中粘结剂含量的10%、20%和30%)的再生沥青混合料的车辙和抗裂性能。结果表明,添加新粘结剂降低了再生沥青混合料的抗车辙性能,但提高了其抗裂性能。此外,对于80%RAP含量且老化5天的再生沥青混合料,最佳新粘结剂含量为1.52%,而90%RAP含量的混合料需要1.23%的新粘结剂。老化10天后,80%RAP含量的再生沥青混合料的最佳新粘结剂含量为1.55%,而90%RAP含量的混合料需要1.28%的新粘结剂。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/acd7/11084739/7f2975cbf755/materials-17-02096-g001.jpg

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验