To clinically evaluate the surface roughness and wear resistance of prefabricated and CAD-CAM milled acrylic resin teeth for complete dentures.
In a cross-over study design, 10 completely edentulous patients were randomly included in this study and given two complete dentures. The first complete denture was made using prefabricated teeth, while the second was constructed using CAD-CAM milled teeth. Following insertion (T0), 3 months (T3), and 6 months (T6), the complete dentures were scanned. Utilizing 3D surface super-imposition techniques, the vertical (2D wear), and volumetric (3D wear) material loss were measured. The hardness of the teeth was evaluated at the time of denture insertion (T0) and then after 6 months (T6) of denture insertion by digital Vickers hardness tester. Statistical analysis was done using SPSS software. Paired groups were compared by paired t-test. Also, a repeated measure test was used. The significant difference was considered if p ≤ 0.05.
The time of denture function was linearly correlated with the wear of the prefabricated and CAD-CAM milled denture tooth. Prefabricated acrylic teeth had significantly more vertical and volumetric wear after 3 and 6 months, compared to CAD-CAM milled denture teeth where p-values were 0.01, 0.009, 0.003, and 0.024, respectively. Additionally, CAD-CAM milled teeth displayed significantly higher hardness values than prefabricated teeth both before and after 6 months of use where p-values were 0.001. After 6 months, all studied teeth showed a decrease in their hardness.
In terms of wear resistance and surface hardness, CAD-CAM milled acrylic resin teeth were superior to prefabricated acrylic resin artificial teeth once the complete denture functions.
临床评估全口义齿预制和CAD-CAM铣削丙烯酸树脂牙的表面粗糙度和耐磨性。
采用交叉研究设计,随机纳入10名全口无牙患者并为其提供两副全口义齿。第一副全口义齿使用预制牙制作,而第二副则使用CAD-CAM铣削牙构建。在义齿戴入后(T0)、3个月(T3)和6个月(T6)时,对全口义齿进行扫描。利用三维表面叠加技术,测量垂直(二维磨损)和体积(三维磨损)材料损失。在义齿戴入时(T0)以及义齿戴入6个月后(T6),通过数字维氏硬度计评估牙齿的硬度。使用SPSS软件进行统计分析。配对组通过配对t检验进行比较。此外,还使用了重复测量检验。若p≤0.05,则认为存在显著差异。
义齿使用时间与预制和CAD-CAM铣削义齿牙的磨损呈线性相关。与CAD-CAM铣削义齿牙相比,预制丙烯酸牙在3个月和6个月后垂直磨损和体积磨损明显更多,其p值分别为0.01、0.009、0.003和0.024。此外,使用6个月前后,CAD-CAM铣削牙的硬度值均显著高于预制牙,p值为0.001。6个月后,所有研究的牙齿硬度均下降。
在耐磨性和表面硬度方面,一旦全口义齿发挥功能,CAD-CAM铣削丙烯酸树脂牙优于预制丙烯酸树脂人工牙。