Bartaria Poorvi, Sharma Priyanka, Sogi H P-Suma, Jain Mansi, Shahi Prinka, Kapoor Roopam
Post Graduate. Maharishi Markandeshwar College of Dental Science and Research.
Reader. Maharishi Markandeshwar College of Dental Science and Research.
J Clin Exp Dent. 2024 Aug 1;16(8):e1027-e1032. doi: 10.4317/jced.61756. eCollection 2024 Aug.
The present study evaluated and compared the microleakage and penetration depth of ACP containing pit and fissure sealant with flowable composite.
Sixty extracted non-carious premolars were categorized into four groups of 15 samples each. Sealant was applied after the Occlusal surfaces of the sample teeth were prophylactically treated with pumice slurry. Later, the teeth were thermocycled and immersed in methylene blue for a period of 24 hours. The samples were buccolingually sectioned and analysed under a stereomicroscope. Statistical analysis was carried out to compare the microleakage and depth of penetration.
Flowable nanocomposite gave comparable results with that of the sealant in terms of microleakage. Nano-hybrid flowable composite performed better with respect to depth of penetration between tested materials with the difference being statistically significant.
Flowable nanocomposite can be considered as a promising substitute for sealing fissures and thus can be endorsed to caries susceptible pediatric patients. Depth of Penetration, Sealants, Microleakage.
本研究评估并比较了含ACP的窝沟封闭剂与流动复合树脂的微渗漏和渗透深度。
将60颗拔除的无龋前磨牙分为四组,每组15个样本。样本牙的咬合面用浮石糊剂进行预防性处理后应用封闭剂。随后,对牙齿进行热循环处理,并在亚甲蓝中浸泡24小时。将样本沿颊舌向切开,在体视显微镜下进行分析。进行统计分析以比较微渗漏和渗透深度。
在微渗漏方面,流动纳米复合树脂与封闭剂的结果相当。在测试材料中,纳米混合流动复合树脂在渗透深度方面表现更好,差异具有统计学意义。
流动纳米复合树脂可被视为一种有前景的窝沟封闭替代材料,因此可推荐给易患龋齿的儿童患者。渗透深度、封闭剂、微渗漏。