Gupta Simran, Gupta Sunil, Mehra Manjul, Gupta Teena, Grover Rashu
Department of Pedodontics, Sri Guru Ram Das Institute of Dental Sciences and Research, Amritsar, Punjab, India.
Int J Clin Pediatr Dent. 2025 Mar;18(3):281-286. doi: 10.5005/jp-journals-10005-3096. Epub 2025 Apr 19.
In achieving clinical success with adhesive materials, bond strength holds significant importance. The goal of testing the strength of the bond is to establish a value for how strong the binding of an adhesive system is to the dental structures. The aim of this study is to comparatively evaluate the shear bond strength of fifth, seventh, and eighth-generations of bonding agents.
Forty-five extracted permanent teeth were allotted into three groups ( = 15), namely, group A: ADPER single bond 2, group B: single bond universal, group C: G-Premio bond. Etchant was applied to the exposed surface, and then adhesive was applied as stated in the manufacturer's instructions, followed by composite (Z350) buildup. The maximum shear force required to debond the specimen was recorded using a universal testing machine. One-way ANOVA test was utilized for statistical comparison at each assessment point, with the significance level set at < 0.05 using SPSS statistical tool.
The maximum shear bond strength was reported for group C, with the mean shear bond strengths of groups A, B, and C being 13.23, 9.66, and 19.21 MPa, respectively.
The newly introduced eighth-generation adhesive showed superior bond strength values compared to the fifth and seventh-generation bonding agents; this difference was statistically significant.
Gupta S, Gupta S, Mehra M, . Comparative Evaluation of Shear Bond Strength of Fifth, Seventh, and Eighth-generation Bonding Agents in Permanent Teeth: An Study. Int J Clin Pediatr Dent 2025;18(3):281-286.
在实现粘结材料的临床成功方面,粘结强度至关重要。测试粘结强度的目的是确定粘结系统与牙齿结构的结合强度值。本研究的目的是比较评估第五代、第七代和第八代粘结剂的剪切粘结强度。
将45颗拔除的恒牙分为三组(每组n = 15),即A组:3M单组分粘结剂第二代;B组:单组分通用粘结剂;C组:G-Premio粘结剂。在暴露的表面涂抹酸蚀剂,然后按照制造商的说明涂抹粘结剂,随后进行复合树脂(Z350)堆塑。使用万能试验机记录使样本脱粘所需的最大剪切力。在每个评估点使用单因素方差分析进行统计比较,使用SPSS统计工具将显著性水平设定为P < 0.05。
C组报告的最大剪切粘结强度最高,A组、B组和C组的平均剪切粘结强度分别为13.23、9.66和19.21MPa。
与第五代和第七代粘结剂相比,新推出的第八代粘结剂显示出更高的粘结强度值;这种差异具有统计学意义。
Gupta S, Gupta S, Mehra M, 。恒牙中第五代、第七代和第八代粘结剂剪切粘结强度的比较评估:一项研究。《国际临床儿科牙科学杂志》2025;18(3):281 - 286。