Brännström M, Torstenson B, Nordenvall K J
J Dent Res. 1984 May;63(5):681-4. doi: 10.1177/00220345840630051501.
Composite resin restorations in cavities are generally associated with the development of a contraction gap during the first minutes after insertion. Enamel-Bond-Concise composite restoration were placed on both approximal sides of extracted pre-molars. The cervical walls of all cavities extended beyond the enamel-cement junction. The enamel walls of one of the cavities in each tooth were acid-etched. The contraction gap was kept air-filled and open at the margin through the use of a special technique. Enamel Bond resin with a fluorescent additive was applied to occlusal and cervical margins of the restorations. The fluorescent resin was "passively" drawn into the gap. In unetched cavities, resin penetrated both cervical and occlusal gaps and some areas of the gap at the axial wall. In cavities with etched enamel, the penetration occurred only at the cervical wall. The distance of penetration from the cervical margin varied from 1 to 6.5 mm, and the width of the contraction gap filled with the fluorescent resin varied from 3.5 to 16 micron. Comparison of the width of the gap at the cervical wall in etched and unetched cavities suggested larger gaps for etched cavities. The method used offers a new technique for the measurement of the contraction gaps around composite resin restorations.
窝洞内的复合树脂修复体在充填后的最初几分钟内通常会出现收缩间隙。在拔除的前磨牙的双侧邻面放置了Enamel - Bond - Concise复合树脂修复体。所有窝洞的颈部壁均延伸至釉质 - 牙骨质界之外。每颗牙齿中一个窝洞的釉质壁进行了酸蚀处理。通过一种特殊技术,使收缩间隙在边缘处保持充满空气且开放。将含有荧光添加剂的Enamel Bond树脂应用于修复体的咬合面和颈部边缘。荧光树脂“被动”地被吸入间隙。在未酸蚀的窝洞中,树脂渗入颈部和咬合面间隙以及轴壁间隙的一些区域。在釉质酸蚀的窝洞中,渗入仅发生在颈部壁。从颈部边缘的渗入距离为1至6.5毫米,充满荧光树脂的收缩间隙宽度为3.5至16微米。酸蚀和未酸蚀窝洞颈部壁间隙宽度的比较表明,酸蚀窝洞的间隙更大。所使用的方法为测量复合树脂修复体周围的收缩间隙提供了一种新技术。