Abstract

Bovine enamels cleaned with citric acid and FeCl3 which had been brushed or ground were joined with PMMA rods with the 4-META/MMA-TBB cement. Their tensile adhesive strength was measured after post-treatments. Stable adhesive strength such as 6.2 MPa was obtained on an enamel which was brushed and washed with an aqueous solution of 10% citric acid-3% FeCl3 for 30 sec. even after a 60 times percolation test between 4 degrees C and 60 degrees C. It is adequate to clinics. The value increased to 16.1 MPa on ground enamel. These results suggest that phosphoric acid etching, essential nowadays, is not necessary for good adhesion to enamel. Monomers with both hydrophobic and hydrophilic groups like 4-META possess affinity with tooth substrates and promote the infiltration of cements into the enamel. The infiltrated monomers polymerized in situ and strong adhesion with the enamel took place. Comparison of the tag length formed in the enamel by cements, MMA-TBB, HNPM/MMA-TBB, Phenyl-P/MMA-TBB and 4-META/MMA-TBB supports this consideration.

摘要

用柠檬酸和三氯化铁清洁过的、经过打磨或研磨的牛牙釉质,使用4-META/MMA-TBB粘结剂与聚甲基丙烯酸甲酯棒材粘结。在进行后处理后测量其拉伸粘结强度。在经过10%柠檬酸-3%三氯化铁水溶液刷洗30秒的牙釉质上,即使在4℃至60℃之间进行60次渗透试验后,仍能获得6.2MPa的稳定粘结强度。这对临床应用来说是足够的。在研磨过的牙釉质上,该值增加到了16.1MPa。这些结果表明,如今必不可少的磷酸酸蚀对于与牙釉质的良好粘结并非必要。像4-META这样具有疏水和亲水基团的单体与牙齿基质具有亲和力,并促进粘结剂渗入牙釉质。渗入的单体原位聚合,与牙釉质形成了牢固的粘结。对MMA-TBB、HNPM/MMA-TBB、Phenyl-P/MMA-TBB和4-META/MMA-TBB粘结剂在牙釉质中形成的标签长度进行比较,支持了这一观点。

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验