Frank C, McDonald D, Wilson J, Eyre D, Shrive N
Department of Surgery, McCaig Centre for Joint Injury and Arthritis Research, University of Calgary, Alberta, Canada.
J Orthop Res. 1995 Mar;13(2):157-65. doi: 10.1002/jor.1100130203.
This study was carried out to quantify the potential associations between material strength and both collagen concentration and pyridinoline collagen crosslink density in the healing medial collateral ligament of the rabbit and to compare these parameters with those of normal ligaments. The right hindlimbs of 24 skeletally mature (12-month-old) New Zealand White rabbits were subjected to a standardized 4 mm midsubstance "gap" injury to the medial collateral ligament. The animals were killed in groups of six at postoperative intervals of 3, 6, 14, or 40 weeks, and the femur-medial collateral ligament-tibia complexes were mechanically tested in tension to failure. Subsequent to mechanical testing, the failure sites of the ligaments were assessed for concentrations of hydroxyproline and hydroxylysyl pyridinoline. Nine additional rabbits served as age-matched normal controls. In healing ligaments, normal collagen concentrations were reached in less than 14 weeks, but the hydroxylysyl pyridinoline crosslink densities remained low and were only 45% of the control values after 40 weeks of healing. Similarly, mechanical values remained much less than the controls. Linear regression analysis of data on scar tissue alone showed a moderately strong positive correlation between hydroxyproline concentration and material strength (r2 = 0.51, p = 0.0001) but no correlation between crosslink density and strength of scar tissue. A similar pattern of correlation was obtained between the elastic modulus of the scar tissue and the biochemical variables, but the r2 values were lower.(ABSTRACT TRUNCATED AT 250 WORDS)
本研究旨在量化兔内侧副韧带愈合过程中材料强度与胶原蛋白浓度及吡啶啉胶原蛋白交联密度之间的潜在关联,并将这些参数与正常韧带的参数进行比较。对24只骨骼成熟(12月龄)的新西兰白兔的右后肢内侧副韧带进行标准化的4mm中部“间隙”损伤。在术后3、6、14或40周时,将动物按每组6只处死,对股骨-内侧副韧带-胫骨复合体进行拉伸力学测试直至破坏。力学测试后,评估韧带断裂部位的羟脯氨酸和羟赖氨酸吡啶啉浓度。另外9只兔子作为年龄匹配的正常对照。在愈合的韧带中,不到14周就达到了正常的胶原蛋白浓度,但羟赖氨酸吡啶啉交联密度仍然很低,愈合40周后仅为对照值的45%。同样,力学值也远低于对照组。仅对瘢痕组织数据进行线性回归分析显示,羟脯氨酸浓度与材料强度之间存在中度强正相关(r2 = 0.51,p = 0.0001),但交联密度与瘢痕组织强度之间无相关性。瘢痕组织的弹性模量与生化变量之间也得到了类似的相关模式,但r2值较低。(摘要截短至250字)