Suppr超能文献

定制托盘材料消毒对几种印模材料系统粘接性能的影响。

Effect of disinfection of custom tray materials on adhesive properties of several impression material systems.

作者信息

Thompson G A, Vermilyea S G, Agar J R

机构信息

Advanced Education Program in Prosthodontics, Walter Reed Army Medical Center, Washington, D.C.

出版信息

J Prosthet Dent. 1994 Dec;72(6):651-6. doi: 10.1016/0022-3913(94)90299-2.

Abstract

The effects of impression tray disinfection procedures on the bond strength of impression-material adhesives to two types of resin trays were evaluated with a tensile test. Autopolymerizing acrylic resin and a visible light-curing resin were formed into one-half inch cubes. A screw eye was attached to each cube before polymerization. Perforated trays were fabricated with stops to maintain an even one-eighth inch of impression material over the resin block. Hooks on the opposite side permitted attachment of the metal plate to a mechanical testing machine. Before adhesive was applied, one third of the resin specimens were immersed in a 1:213 iodophor solution; one third in a 10% sodium hypochlorite solution, and one third were kept in the "as fabricated" condition. Polysulfide, polyether, and polyvinyl siloxane impression material-adhesive systems were evaluated. The resin-impression material-metal plate couples were attached to a mechanical testing machine and tensile forces were applied at a separation rate of 5 inches per minute. Mean values for adhesive strength ranged from 3.49 kg/cm2 for the autopolymerizing acrylic resin/iodophor/polyether combination to 10.55 kg/cm2 for the autopolymerizing acrylic resin/untreated/polyvinyl siloxane combination. Differences were detected among materials and disinfecting procedure. Clinically, disinfection of resin trays may adversely affect retention of the impression material to the tray.

摘要

通过拉伸试验评估了印模托盘消毒程序对两种树脂托盘上印模材料粘合剂粘结强度的影响。将自凝丙烯酸树脂和可见光固化树脂制成半英寸的立方体。在聚合前,在每个立方体上连接一个螺丝孔眼。制作带挡块的穿孔托盘,以使树脂块上的印模材料均匀保持八分之一英寸厚。另一侧的挂钩允许将金属板连接到机械试验机上。在施加粘合剂之前,将三分之一的树脂样本浸入1:213碘伏溶液中;三分之一浸入10%次氯酸钠溶液中,三分之一保持“制作完成时”的状态。评估了聚硫橡胶、聚醚和聚乙烯基硅氧烷印模材料 - 粘合剂系统。将树脂 - 印模材料 - 金属板组件连接到机械试验机上,并以每分钟5英寸的分离速率施加拉力。粘合剂强度的平均值范围为自凝丙烯酸树脂/碘伏/聚醚组合的3.49 kg/cm²至自凝丙烯酸树脂/未处理/聚乙烯基硅氧烷组合的10.55 kg/cm²。在材料和消毒程序之间检测到差异。临床上,树脂托盘的消毒可能会对印模材料在托盘上的固位产生不利影响。