Caries Res. 1995;29(1):14-9. doi: 10.1159/000262034.
Recently, several papers investigated the linear dimensional changes in dentine after air-drying. This paper pertains to weight changes, volume changes, and density changes caused by air-drying of sound and demineralized intact dentine. The densities of sound and artificially demineralized human coronal dentine were measured in the wet state and after various drying periods of up to 24 h. The volume was assessed either by means of a pyknometer (wet samples) or by means of dimension measurements. The air-drying experiments were done using a Mettler thermobalance at room temperature. The density of wet sound coronal dentine was found to be 2.24 +/- 0.12 g.cm-3; the value of wet demineralized dentine was about 1.6 g.cm-3. The data show that previously published density values of powdered sound dentine may have been influenced by powdering effects, air-drying, and air inclusion. In whole demineralized air-dried dentine, air inclusion can be very severe: up to 30% by volume. The results show furthermore that in demineralized dentine we have two drying stages: during the first one (up to about 10 min of air-drying), the lesions shrink about 23%, while a main part of the water in the lesion evaporates, and air is incorporated into the tissue; during the second stage (drying longer than 10 min), the lesions hardly shrink anymore, but water is evaporated mainly from underlying sound dentine, followed by air incorporation.
最近,有几篇论文研究了空气干燥后牙本质的线性尺寸变化。本文涉及健康完整牙本质和脱矿完整牙本质空气干燥引起的重量变化、体积变化和密度变化。在湿态以及长达24小时的不同干燥时间段后,测量了健康的和人工脱矿的人冠部牙本质的密度。通过比重瓶(湿样本)或尺寸测量来评估体积。空气干燥实验在室温下使用梅特勒热重天平进行。发现湿态健康冠部牙本质的密度为2.24±0.12 g·cm⁻³;湿态脱矿牙本质的值约为1.6 g·cm⁻³。数据表明,先前发表的粉末状健康牙本质的密度值可能受到粉末化效应、空气干燥和空气夹杂的影响。在完全脱矿的空气干燥牙本质中,空气夹杂可能非常严重:体积可达30%。结果还表明,在脱矿牙本质中存在两个干燥阶段:在第一个阶段(空气干燥长达约10分钟),病变收缩约23%,同时病变中的大部分水分蒸发,空气进入组织;在第二个阶段(干燥时间超过10分钟),病变几乎不再收缩,但水分主要从下方的健康牙本质中蒸发,随后空气进入。