Suppr超能文献

Analysis of debond rates of resin-bonded prostheses.

作者信息

Boyer D B, Williams V D, Thayer K E, Denehy G E, Diaz-Arnold A M

机构信息

Department of Operative Dentistry, College of Dentistry, University of Iowa, Iowa City 52242.

出版信息

J Dent Res. 1993 Aug;72(8):1244-8. doi: 10.1177/00220345930720081401.

Abstract

Debonding rates of 164 resin-bonded prostheses (RBP) placed from 1974 to 1985 were examined at recall. The yearly debond rates were calculated, the cumulative probability of failure was determined for the debonded RBPs, and Weibull distribution parameters were determined. For perforated prostheses, there was a high initial debond rate, followed by slowly decreasing rates for about 5 years. Increasing rates after 5 years indicated the beginning of wear-out. The Weibull parameters for the wear-out period of the perforated prostheses were: characteristic life = 128 (SE = 2) months, modulus = 1.27 (0.06), and threshold parameter = 0. Data were available for etched frameworks for 6 years and showed decreasing debond rates during this time. The characteristic life of the etched bridges was 318 (84) months. The cumulative failure data were also modeled with a cubic polynomial distribution that resulted in a U-shaped hazard function.

摘要

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验