Navarro M F, Franco E B, Bastos P A, Teixeira L C, Carvalho R M
Department of Operative Dentistry, University of São Paulo, School of Dentistry, Bauru, Brazil.
Quintessence Int. 1996 May;27(5):315-20.
This study evaluated 30 gallium alloy (Gallium alloy GF) and 31 amalgam (Dispersalloy) restorations over a period of 8 months in both Class I and Class II cavity preparations in 28 human subjects. At baseline, all gallium alloy and amalgam restorations were considered acceptable (Alfa) in terms of caries, anatomic form, marginal adaptation, surface texture, and bulk fracture. Postoperative sensitivity was reported in 67% of the gallium alloy restorations and in 29% of the amalgam restorations. At 8 months, 61% of the gallium alloy restorations were rated Beta for marginal adaptation, and all restorations exhibited tarnish and corrosion. With a few exceptions, the amalgam restorations were rated Alfa for those criteria. Three gallium alloy restorations had to be replaced during the evaluation period because of severe postoperative sensitivity and 39% of gallium restorations still presented some sensitivity at 8 months. Additional problems exhibited by gallium restorations were tooth fractures, tooth cracks, and marginal whitening.
本研究对28名受试者的I类和II类洞型制备中的30个镓合金(镓合金GF)修复体和31个汞合金(Dispersalloy)修复体进行了为期8个月的评估。基线时,所有镓合金和汞合金修复体在龋齿、解剖形态、边缘适应性、表面质地和整体断裂方面均被认为是可接受的(Alfa)。67%的镓合金修复体和29%的汞合金修复体报告有术后敏感症状。8个月时,61%的镓合金修复体边缘适应性被评为Beta级,所有修复体均出现了变色和腐蚀。除少数例外,汞合金修复体在这些标准方面被评为Alfa级。在评估期间,有3个镓合金修复体因严重的术后敏感症状而不得不更换,8个月时39%的镓合金修复体仍有一些敏感症状。镓合金修复体还出现了牙齿折断、牙齿裂纹和边缘变白等其他问题。