This study evaluated the effect of dentin surface treatment on shear bond strengths of two light- cured glass ionomer restorative materials to dentin. Cylinders of Fuji II LC and VariGlass VLC were bonded to dentin surfaces that were untreated, treated with a 10% polyacrylic acid (GC Conditioner), or treated with a dentin bonding agent primer (Prisma Universal Bond 3 Primer). Specimens were thermocycled and tested in shear at 7 days. Data for each restorative material were subjected to one way ANOVA and Tukey's procedure at the 0.05 probability level. For Fuji II LC, mean bond strength to conditioner-treated dentin was significantly higher than mean bond strength to primer-treated dentin and to untreated dentin. For VariGlass VLC, mean bond strength to primer-treated dentin was significantly higher than mean bond strength to untreated dentin. Bond strengths to primer-treated dentin and conditioner-treated dentin were not significantly different.
本研究评估了牙本质表面处理对两种光固化玻璃离子修复材料与牙本质之间剪切粘结强度的影响。将富士II LC和VariGlass VLC圆柱体粘结到未经处理、用10%聚丙烯酸处理(GC调节剂)或用牙本质粘结剂底漆处理(Prisma通用粘结3底漆)的牙本质表面。样本进行热循环处理,并在7天时进行剪切测试。每种修复材料的数据在0.05概率水平下进行单因素方差分析和Tukey检验。对于富士II LC,与经调节剂处理的牙本质的平均粘结强度显著高于与经底漆处理的牙本质和未经处理的牙本质的平均粘结强度。对于VariGlass VLC,与经底漆处理的牙本质的平均粘结强度显著高于与未经处理的牙本质的平均粘结强度。与经底漆处理的牙本质和经调节剂处理的牙本质的粘结强度没有显著差异。