Lekovic V, Klokkevold P R, Kenney E B, Dimitrijelic B, Nedic M, Weinlaender M
University of Belgrade, School of Dentistry, Yugoslavia.
J Periodontol. 1998 Jan;69(1):54-61. doi: 10.1902/jop.1998.69.1.54.
This study evaluated and compared four different barrier membrane materials used to treat class II mandibular premolar and molar furcations in seven dogs with naturally occurring periodontitis. Five class II furcation defects in each animal were randomly assigned to one of four experimental groups or to a control group. Each defect was treated by surgical debridement, root planing, and barrier membrane coverage with one of the four test materials or no barrier membrane (control). Thus, each animal served as its own control. Following 6 months of healing, block sections were used to histologically measure the amount of regenerated tissue and stereometrically enumerate the inflammatory cell infiltration observed with each of the treatment modalities. The four barrier membrane materials (polycarbonate filter, silicone rubber, expanded polytetrafluoroethylene, and polycaprolactone) all provided a wound healing environment that promoted new cementum formation, with mean values ranging from 1.96 +/- 0.031 mm to 2.18 +/- 0.015 mm, and facilitated alveolar bone regeneration, with mean values ranging from 1.18 +/- 0.019 mm to 1.44 +/- 0.014 mm. Control-treated sites showed mean values of only 0.24 +/- 0.007 mm new cementum formation and 0.32 +/- 0.017 mm bone fill. Polycarbonate filter and polycaprolactone membrane barriers elicited a significantly greater chronic inflammatory cell response of lymphocyte and plasma cell infiltrates as compared to expanded polytetrafluoroethylene and silicone rubber, which were comparable to control-treated sites.
本研究评估并比较了四种不同的屏障膜材料,用于治疗7只患有自然发生牙周炎的犬的II类下颌前磨牙和磨牙根分叉病变。每只动物的5个II类根分叉缺损被随机分配到四个实验组之一或一个对照组。每个缺损均通过手术清创、根面平整,并使用四种测试材料之一覆盖屏障膜或不使用屏障膜(对照组)进行治疗。因此,每只动物自身作为对照。愈合6个月后,使用块状切片进行组织学测量再生组织的量,并通过立体测量法计数每种治疗方式下观察到的炎性细胞浸润情况。四种屏障膜材料(聚碳酸酯滤膜、硅橡胶、膨体聚四氟乙烯和聚己内酯)均提供了促进新牙骨质形成的伤口愈合环境,平均值在1.96±0.031mm至2.18±0.015mm之间,且促进了牙槽骨再生,平均值在1.18±0.019mm至1.44±0.014mm之间。对照组处理的部位新牙骨质形成的平均值仅为0.24±0.007mm,骨填充量为0.32±0.017mm。与膨体聚四氟乙烯和硅橡胶相比,聚碳酸酯滤膜和聚己内酯膜屏障引发了明显更强的淋巴细胞和浆细胞浸润的慢性炎性细胞反应,而膨体聚四氟乙烯和硅橡胶与对照组处理部位相当。