Deng X, Yue Y, Gao Z
Department of Chemistry, Fudan University, Shanghai, 200433, People's Republic of China
J Colloid Interface Sci. 1998 Oct 1;206(1):52-57. doi: 10.1006/jcis.1998.5645.
Carbon-silica composite adsorbents with high surface area and pore volume were prepared from natural elutrilithe. The elutrilithe was chemically activated with K2CO3 at 1123 K and then dissolved in water. The textural and adsorptive properties of the composite adsorbents can be adjusted by varying the pH and concentration of the sol mixture and the gel aging temperature. Composite adsorbents prepared at low concentration have high adsorption capacities for both water (43.4%) and cyclohexane (32.0%), exceeding those of ordinary commercial silica gel and active carbon. The adsorbents prepared at high concentration are more hydrophobic in nature, with adsorption capacities for water and cyclohexane of 18.5 and 41.5%, respectively. The composite adsorbents are resistant to repetitive adsorption and regeneration cycles. Copyright 1998 Academic Press.
以天然漂灰土为原料制备了具有高比表面积和孔体积的碳-硅复合吸附剂。将漂灰土在1123 K下用碳酸钾进行化学活化,然后溶解于水中。通过改变溶胶混合物的pH值、浓度以及凝胶老化温度,可以调节复合吸附剂的结构和吸附性能。低浓度下制备的复合吸附剂对水(43.4%)和环己烷(32.0%)均具有高吸附容量,超过了普通商业硅胶和活性炭。高浓度下制备的吸附剂本质上更疏水,对水和环己烷的吸附容量分别为18.5%和41.5%。该复合吸附剂耐重复吸附和再生循环。版权所有1998年学术出版社。