Oper Dent. 1999 Mar-Apr;24(2):96-102.
The purpose of this study was to investigate the effect of various dentin acid treatments on the tensile bond strength of resin composite to dentin, mediated by Prisma Universal Bond 2. Acid solutions (maleic acid, Na-EDTA, phosphoric acid, citric acid/ferric chloride) were applied to dentin surfaces for 15 seconds or 60 seconds, and tensile bond strengths evaluated. For all acids, there was a significant difference in bond strength for the two treatment times; for phosphoric acid and citric acid/ferric chloride, the 15-second application resulted in a higher bond strength, while the reverse was true for Na-EDTA (sodium-EDTA) and maleic acid. The highest bond strength (19.6 MPa) was associated with 15-second citric acid/ferric chloride application, and the lowest bond strength (5.6 MPa) with 60-second application of citric acid/ferric chloride. The bond strengths with 60-second citric acid/ferric chloride (5.6 MPa), 15-second Na-EDTA (5.8 MPa), and 60-second phosphoric acid (6.3 MPa) were not significantly different from the control (5.7 MPa).
本研究的目的是调查由Prisma Universal Bond 2介导的各种牙本质酸处理对树脂复合材料与牙本质拉伸粘结强度的影响。将酸溶液(马来酸、乙二胺四乙酸钠、磷酸、柠檬酸/氯化铁)应用于牙本质表面15秒或60秒,并评估拉伸粘结强度。对于所有酸,两种处理时间的粘结强度存在显著差异;对于磷酸和柠檬酸/氯化铁,15秒的处理导致更高的粘结强度,而乙二胺四乙酸钠(Na-EDTA)和马来酸则相反。最高粘结强度(19.6MPa)与15秒的柠檬酸/氯化铁处理相关,最低粘结强度(5.6MPa)与60秒的柠檬酸/氯化铁处理相关。60秒的柠檬酸/氯化铁(5.6MPa)、15秒的乙二胺四乙酸钠(5.8MPa)和60秒的磷酸(6.3MPa)的粘结强度与对照组(5.7MPa)无显著差异。