Suppr超能文献

新型可生物降解环装置用于机械性微血管吻合的实验研究

Experimental study of mechanical microvascular anastomosis with new biodegradable ring device.

作者信息

Joji S, Muneshige H, Ikuta Y

机构信息

Department of Orthopaedic Surgery, Hiroshima University School of Medicine, Hiroshima, Japan.

出版信息

Br J Plast Surg. 1999 Oct;52(7):559-64. doi: 10.1054/bjps.1999.3131.

Abstract

The commercially available mechanical vascular anastomotic device with ring-pin technique employs polyethylene rings and stainless steel pins, but even after healing of the anastomotic site, the ring remains. To resolve this disadvantage, the ring material was replaced by biodegradable material, and a ring coupling device was fabricated. This new ring was used to anastomose the femoral vein of rabbits, and morphological observations were made macroscopically and by light and scanning electron microscopy. Of the 58 anastomosed veins, 54 were patent, giving a patency rate of 92.9%. The ring was largely absorbed 15 weeks after anastomosis and completely after 30 weeks. Histologically, re-endothelialisation was observed in 1 week. Infiltration of inflammatory cells was significant around the ring at 3 weeks, but inflammation subsided within 6 weeks. There were no findings indicating adverse effects of the stainless steel pins remaining outside the vascular wall.

摘要

市售的采用环钉技术的机械血管吻合装置使用聚乙烯环和不锈钢钉,但即使吻合部位愈合后,环仍会留存。为解决这一缺点,将环材料替换为可生物降解材料,并制作了一种环连接装置。将这种新环用于兔股静脉吻合,并进行大体观察以及光镜和扫描电镜形态学观察。在58条吻合静脉中,54条通畅,通畅率为92.9%。吻合后15周环大部分被吸收,30周后完全吸收。组织学检查显示,1周时可见再内皮化。3周时环周围炎症细胞浸润明显,但炎症在6周内消退。未发现血管壁外留存的不锈钢钉有不良反应的迹象。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验