Vlasko-Vlasov V K, Lin Y K, Miller D J, Welp U, Crabtree G W, Nikitenko V I
Argonne National Laboratory, 9700 South Cass Avenue, Argonne, Illinois 60439, USA.
Phys Rev Lett. 2000 Mar 6;84(10):2239-42. doi: 10.1103/PhysRevLett.84.2239.
The spontaneous formation of twins in La(2/3)Ca(1/3)MnO3 films below T(S) approximately 105 K is observed by a magneto-optical technique. The twins are revealed as stripes along the {110} directions where magnetization tilts out of the film plane due to the stresses in twins. Their appearance is associated with a martensitic phase transition in the film triggered by the cubic-to-tetragonal transition in the SrTiO3 substrate. It is found that magnetization of the films proceeds by inhomogeneous rotation of magnetic moments. This is due to the presence of microscopic structural inhomogeneities. Their dominating role in the low-temperature transport can explain small effects of the transition at T(S) on the resistivity.
通过磁光技术观察到,在温度低于约105K的T(S)时,La(2/3)Ca(1/3)MnO3薄膜中会自发形成孪晶。孪晶表现为沿{110}方向的条纹,由于孪晶中的应力,磁化强度会倾斜出薄膜平面。它们的出现与SrTiO3衬底中由立方相向四方相转变引发的薄膜马氏体相变有关。研究发现,薄膜的磁化是通过磁矩的非均匀旋转进行的。这是由于存在微观结构不均匀性。它们在低温输运中的主导作用可以解释T(S)处的转变对电阻率的微小影响。