Tognetto D, Toto L, Ravalico G
Eye Clinic, University of Trieste, Trieste, Italy.
J Cataract Refract Surg. 2000 Oct;26(10):1560-4. doi: 10.1016/s0886-3350(00)00415-6.
A series of pits varying in depth and size appeared on the anterior surface of hydrogel intraocular lenses (IOLs) soon after they were implanted. In all cases, the pits increased in size but not in number during a 1 year follow-up. The origin of the pit defects is unknown and does not seem related to inflammatory or lens epithelial cell activity. Hydration of the IOL could be a cause even if a manufacturing defect were present. This IOL surface alteration did not seem to impair visual function or cause visual disturbances.
水凝胶人工晶状体(IOL)植入后不久,其前表面就出现了一系列深度和大小各异的凹坑。在所有病例中,这些凹坑在1年的随访期间大小增加但数量未增加。凹坑缺陷的起源尚不清楚,似乎与炎症或晶状体上皮细胞活动无关。即使存在制造缺陷,IOL的水化也可能是一个原因。这种IOL表面改变似乎并未损害视觉功能或引起视觉障碍。