This in vitro study compared the force-deflection behavior of 8 superelastic nickel-titanium orthodontic wires (0.017 x 0.025 in) under controlled moment and temperature. To simulate leveling a lateral incisor, brackets and first molar tubes without tip and angulation were used. The wires (n = 5) were ligated into stainless steel brackets attached to a plastic jig to simulate a mandibular arch. A testing machine (Instron) applied deflections of 0.2 to 2.0 mm at 35 degrees C in the lateral incisor area. Force-deflection diagrams were determined from the passive position to an activation of 2 mm and then during deactivation. Forces on deactivation at a deflection of 1 mm were compared by analysis of variance. Significant differences (P < .05) in forces were observed among wires. All wires exhibited superelastic behavior, but in stratified loading levels.
这项体外研究比较了8根超弹性镍钛正畸丝(0.017×0.025英寸)在受控力矩和温度下的力-挠度行为。为模拟整平侧切牙,使用了无转矩和角度的托槽及第一磨牙管。将5根正畸丝结扎到连接在塑料夹具上的不锈钢托槽中,以模拟下颌牙弓。一台测试机(英斯特朗)在35℃下于侧切牙区域施加0.2至2.0毫米的挠度。测定从被动位置到激活2毫米以及随后去激活过程中的力-挠度图。通过方差分析比较了在1毫米挠度下去激活时的力。在各正畸丝之间观察到力有显著差异(P<0.05)。所有正畸丝均表现出超弹性行为,但处于分层加载水平。