Sarkar N K, Greener E H
Biomater Med Devices Artif Organs. 1975;3(4):429-37. doi: 10.3109/10731197509118634.
Anodic polarization measurements of Dispersalloy amalgam in Ringer's solution have shown that its electrochemical behavior is significantly altered by the aging of the alloy at room temperature. Amalgams fabricated from aged alloy are characterized by polarization profiles associated with the presence of Sn7 Hg (gamma2) and Cu-Sn (Cu/Sn less than 3) whereas polarization profiles of amalgams fabricated from relatively fresh alloys are free of current density peaks associated with both of these phases. This aging effect has been attributed to the room temperature oxidation of Ag-Cu eutectic, a component of Dispersalloy. Such oxidation, it has been hypothesized, hinders amalgamation, impairs the effective role of the Ag-Cu eutectic in eliminating the gamma2- phase, and produces corrosion-prone Cu-Sn intermetallics (Cu/Sn less than 3).
在林格氏溶液中对Dispersalloy汞合金进行的阳极极化测量表明,室温下合金的时效会显著改变其电化学行为。由时效合金制成的汞合金的特征在于与Sn7Hg(γ2)和Cu-Sn(Cu/Sn小于3)的存在相关的极化曲线,而由相对新鲜的合金制成的汞合金的极化曲线没有与这两个相相关的电流密度峰值。这种时效效应归因于Dispersalloy的一种成分Ag-Cu共晶在室温下的氧化。据推测,这种氧化会阻碍汞齐化,损害Ag-Cu共晶在消除γ2相方面的有效作用,并产生易腐蚀的Cu-Sn金属间化合物(Cu/Sn小于3)。