用于正畸粘结的等离子弧固化灯。

Plasma arc curing lights for orthodontic bonding.

作者信息

Klocke Arndt, Korbmacher Heike M, Huck Lothar G, Kahl-Nieke Bärbel

机构信息

Department of Orthodontics, College of Dentistry, University of Hamburg, UKE, Martinistrasse 52, 20246 Hamburg, Germany.

出版信息

Am J Orthod Dentofacial Orthop. 2002 Dec;122(6):643-8. doi: 10.1067/mod.2002.126897.

Abstract

Xenon plasma arc lights were introduced recently for light-cured orthodontic bonding. Compared with a conventional tungsten-quartz-halogen light source, these high-intensity lights promise a dramatic reduction in curing time. The purpose of this in vitro investigation was to evaluate bond strength with 2 commercially available plasma arc lights and reduced curing intervals. Brackets were bonded to 150 extracted human teeth (75 premolars, 75 incisors) with a composite adhesive. Intervals of 2 and 6 seconds were used for curing with the plasma arc lights; a control group was bonded with a halogen light source and 20 seconds of light exposure per bracket. Bond strength testing was performed with a universal testing machine. A substantial reduction in curing time was possible with both plasma arc units. Significantly lower bond strength values were found for premolar brackets bonded with plasma arc curing lights and the shortest curing interval of 2 seconds compared with the longer curing time of 6 seconds or the standard curing time with the halogen light. Although 2 seconds of curing might be adequate to achieve acceptable bond strength values for the incisors, the Weibull analysis indicated a higher probability of bond failure for premolar brackets in particular. Six seconds of curing time is recommended for bonding stainless steel brackets with xenon plasma arc light sources.

摘要

氙气等离子弧光灯最近被引入用于光固化正畸粘结。与传统的钨-石英-卤素光源相比,这些高强度灯有望显著缩短固化时间。本体外研究的目的是评估两种市售等离子弧光灯以及缩短固化时间间隔时的粘结强度。使用复合粘合剂将托槽粘结到150颗拔除的人牙上(75颗前磨牙,75颗切牙)。使用等离子弧光灯固化的时间间隔为2秒和6秒;对照组使用卤素光源,每个托槽光照20秒。使用万能试验机进行粘结强度测试。两种等离子弧装置都能大幅缩短固化时间。与6秒的较长固化时间或卤素灯的标准固化时间相比,用等离子弧固化灯和最短2秒的固化时间粘结的前磨牙托槽的粘结强度值明显较低。虽然2秒的固化时间可能足以使切牙获得可接受的粘结强度值,但威布尔分析表明,尤其是前磨牙托槽粘结失败的可能性更高。建议使用氙气等离子弧光源粘结不锈钢托槽时的固化时间为6秒。