Tuncan Mustafa, Tuncan Ahmet, Cetin Altan
Department of Civil Engineering, Anadolu University, Iki Eylul Kampusu, 26470, Eskisehir, Turkey.
Waste Manag Res. 2003 Apr;21(2):83-92. doi: 10.1177/0734242X0302100202.
The purpose of this study was to investigate (a) the effects of rubber and plastic concentrations and rubber particle sizes on properties of asphalt cement, (b) on properties of asphalt concrete specimens and (c) the effects of fly ash, marble powder, rubber powder and petroleum contaminated soil as filler materials instead of stone powder in the asphalt concrete specimens. One type of limestone aggregate and one penetration-graded asphalt cement (75-100) were used. Three concentrations of rubber and plastic (i.e. 5%, 10% and 20% of the total weight of asphalt cement), three rubber particle sizes (i.e. No. 4 [4.75mm] - 20 [0.85 mm], No. 20 [0.85mm] - 200 [0.075mm] and No. 4 [4.75mm] - 200 [0.075mm]) and one plastic particle size (i.e. No. 4 [4.75mm] - 10 [2.00mm]) were also used. It was found that while the addition of plastic significantly increased the strength of specimens, the addition of rubber decreased it. No. 4 [4.75mm] - 200 [0.075mm] rubber particles showed the best results with respect to the indirect tensile test. The Marshall stability and indirect tensile strength properties of plastic modified specimens increased. Marble powder and fly ash could be used as filler materials instead of stone powder in the asphalt concrete pavement specimens.
(a)橡胶和塑料浓度以及橡胶颗粒尺寸对沥青胶浆性能的影响;(b)对沥青混凝土试件性能的影响;以及(c)在沥青混凝土试件中,用粉煤灰、大理石粉、橡胶粉和石油污染土壤作为填充材料替代石粉的效果。使用了一种石灰岩集料和一种针入度分级的沥青胶浆(75-100)。还使用了三种橡胶和塑料浓度(即沥青胶浆总重量的5%、10%和20%)、三种橡胶颗粒尺寸(即4号[4.75毫米]-20号[0.85毫米]、20号[0.85毫米]-200号[0.075毫米]和4号[4.75毫米]-200号[0.075毫米])以及一种塑料颗粒尺寸(即4号[4.75毫米]-10号[2.00毫米])。研究发现,虽然添加塑料显著提高了试件的强度,但添加橡胶却降低了强度。就间接拉伸试验而言,4号[4.75毫米]-200号[0.075毫米]橡胶颗粒显示出最佳结果。塑料改性试件的马歇尔稳定性和间接拉伸强度性能有所提高。在沥青混凝土路面试件中,大理石粉和粉煤灰可以用作填充材料替代石粉。