牙科汞合金与口腔环境之间的相互作用。

Interactions between dental amalgams and the oral environment.

作者信息

Marek M

机构信息

School of Materials Engineering, Georgia Institute of Technology, Atlanta 30332.

出版信息

Adv Dent Res. 1992 Sep;6:100-9. doi: 10.1177/08959374920060010101.

Abstract

Dental amalgam fillings interact in a complex way with the environment in the oral cavity as they are subjected to chemical, biological, mechanical, and thermal forces. These forces change the restoration's appearance and properties, while metal ions, amalgam debris, non-metallic corrosion products, and mercury vapor are released into the oral cavity. The phenomena and conditions that affect the amalgam/environment interaction include the chemistry and biochemistry of the environment, formation of biofilms on the amalgam surfaces, existence of localized corrosion cells, galvanic contacts with other metallic restorations, abrasion during mastication, and synergistic effects of the different forces. Corrosion processes result in a degradation of the functional amalgam properties, while tarnishing reactions cause discoloration. Corrosion degradation of amalgam fillings is due mainly to localized corrosion cells in pores and crevices. Corrosion on occlusal surfaces is accelerated by abrasion during mastication, which removes the protective surface films. The average total amounts of metal species, including mercury, released per day in vivo from a restoration have not been determined. Much of the reported indirect evidence for high mercury release rates is either unreliable or controversial. A more detailed investigation is needed and will require the development of more sophisticated techniques of sampling in vivo, as well as both experimental and theoretical modeling in vitro.

摘要

牙科汞合金填充物在口腔环境中会受到化学、生物、机械和热力的作用,其相互作用方式复杂。这些作用力会改变修复体的外观和性能,同时金属离子、汞合金碎屑、非金属腐蚀产物和汞蒸气会释放到口腔中。影响汞合金与环境相互作用的现象和条件包括环境的化学和生物化学性质、汞合金表面生物膜的形成、局部腐蚀电池的存在、与其他金属修复体的电偶接触、咀嚼过程中的磨损以及不同作用力的协同效应。腐蚀过程会导致汞合金功能性能的退化,而 tarnishing 反应会导致变色。汞合金填充物的腐蚀退化主要是由于孔隙和缝隙中的局部腐蚀电池。咀嚼过程中的磨损会加速咬合面的腐蚀,磨损会去除保护表面膜。尚未确定修复体在体内每天释放的包括汞在内的金属物种的平均总量。所报道的许多关于高汞释放率的间接证据要么不可靠,要么存在争议。需要进行更详细的调查,这将需要开发更复杂的体内采样技术,以及体外实验和理论建模。

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验