Fatt I, Weissman B A
School of Optometry, University of California, Berkeley.
Optom Vis Sci. 1992 Dec;69(12):931-5. doi: 10.1097/00006324-199212000-00004.
The oxygen transmissibility of a contact lens is defined as its oxygen permeability (Dk) divided by its thickness (L). Transmissibility can be obtained from separate measurements of Dk and L, or from a single measurement of oxygen flux through the lens (as for example by the polarographic method). Dk/L of hydrogel contact lenses with optical power measured by the polarographic method was compared with Dk/L calculated from separate measurements of Dk and L. Polarographic sensors of different cathode diameters were used to show the effect of the area over which the flux is measured on the observed Dk/L. Dk/L from oxygen flux measured by the polarographic sensor was found to be a function of the optical power of the lens and cathode diameter. Dk/L calculated from separately determined Dk and L for optically powered lenses was found to be a function of Dk and the choice of L (central or average).
隐形眼镜的透氧性定义为其氧气透过系数(Dk)除以其厚度(L)。透氧性可以通过分别测量Dk和L获得,或者通过对穿过镜片的氧通量进行单次测量(例如通过极谱法)获得。将通过极谱法测量的具有屈光力的水凝胶隐形眼镜的Dk/L与通过分别测量Dk和L计算得到的Dk/L进行比较。使用不同阴极直径的极谱传感器来显示测量通量的面积对观察到的Dk/L的影响。发现通过极谱传感器测量的氧通量得到的Dk/L是镜片屈光力和阴极直径的函数。对于有屈光力的镜片,由分别测定的Dk和L计算得到的Dk/L是Dk和L的选择(中心值或平均值)的函数。