Abstract

Currently commercially available acrylic bone cements lack adequate radiopacity and viscosity when they are used in percutaneous vertebroplasty (PVP). In this work improved formulations of radiopaque and injectable poly(methyl methacrylate) bone cements were prepared with different amounts (10-50 wt.%) of BaTiO3 or SrTiO3 particles as the radiopaque agent. Two sets of cements were prepared by using untreated or silanated radiopaque particles, respectively. The influence of the content and nature of the radiopaque agent as well as its silanation with 3-(trimethoxysilyl) propyl methacrylate (gamma-MPS), on the curing parameters, residual monomer content, radiopacity, mechanical properties, and injectability of the resulting materials, was examined. Doughing and setting times, maximum temperature, and compressive strength of all formulations fulfilled the requirements of standard specifications, with values of peak temperature in the range 57-72 degrees C and those of compressive strength between 114 and 135 MPa. Formulations containing at least 20 wt.% BaTiO3 or SrTiO3 had radiopacities equal to or greater than that corresponding to 2 mm of Al as required for surgical plastics. Injectability of any of the formulations provided 75-80 wt.% of the total mass manually injected through a conventional biopsy needle 4 min after mixing. Silanation of the BaTiO3 or SrTiO3 particles led to formulations with improved mechanical properties and injectability compared to those obtained with the untreated fillers.

摘要

目前市售的丙烯酸骨水泥在经皮椎体成形术(PVP)中使用时,缺乏足够的射线不透性和粘度。在这项工作中,制备了具有不同含量(10 - 50 wt.%)的钛酸钡或钛酸锶颗粒作为射线不透性剂的射线不透性且可注射的聚甲基丙烯酸甲酯骨水泥的改进配方。分别使用未处理的或硅烷化的射线不透性颗粒制备了两组水泥。研究了射线不透性剂的含量和性质及其用甲基丙烯酸3 -(三甲氧基甲硅烷基)丙酯(γ - MPS)进行硅烷化对所得材料的固化参数、残留单体含量、射线不透性、机械性能和可注射性的影响。所有配方的面团期和凝固时间、最高温度和抗压强度均符合标准规格要求,峰值温度值在57 - 72℃范围内,抗压强度值在114 - 135 MPa之间。含有至少20 wt.%钛酸钡或钛酸锶的配方具有等于或大于手术塑料制品所需的相当于2 mm铝的射线不透性。任何配方在混合4分钟后通过传统活检针手动注射的总质量中,可注射性提供75 - 80 wt.%。与使用未处理填料获得的配方相比,钛酸钡或钛酸锶颗粒的硅烷化导致配方具有改善的机械性能和可注射性。