Okamura Mitsunobu, Chen Ker-Kong, Kakigawa Hiroshi, Kozono Yoshio
Department of Materials Science, Kyushu Dental College, Manazuru, Kokurakita, Kitakyushu, Japan.
Dent Mater J. 2004 Jun;23(2):180-3. doi: 10.4012/dmj.23.180.
A densely sintered high-purity alumina has been successfully utilized as a coping for all-ceramic crown. In order to apply the alumina coping to the porcelain laminate veneer restoration for the discolored teeth, the present study evaluated its masking ability when it was thinner than the proposed thickness for the crown. Colorimetric examination was performed on white and black backgrounds for the 0.7 mm thick porcelain laminate veneer with 0.40 or 0.25 mm thick alumina coping and 0.7 mm thick porcelain without coping. With the presence of the coping, the porcelain appeared significantly lighter. Judging from the calculated color differences delta E and the literature, it was suggested that the masking ability of the alumina coping would be sufficient with a 0.25 mm thickness for the porcelain laminate veneer for heavily discolored teeth.
一种致密烧结的高纯度氧化铝已成功用作全瓷冠的内冠。为了将氧化铝内冠应用于变色牙的瓷贴面修复,本研究评估了其厚度小于冠部建议厚度时的遮色能力。在白色和黑色背景上,对厚度为0.7mm的瓷贴面搭配0.40mm或0.25mm厚的氧化铝内冠以及无内冠的0.7mm厚瓷进行了比色检查。有内冠时,瓷显得明显更亮。从计算出的色差ΔE和文献判断,对于严重变色牙的瓷贴面,氧化铝内冠厚度为0.25mm时其遮色能力可能足够。