El Zohairy Ahmed A, De Gee Anton J, Mohsen Mohamed M, Feilzer Albert J
Department of Dental Materials Science, Academic Center for Dentistry Amsterdam (ACTA), Amsterdam, Netherlands.
Dent Mater. 2005 Feb;21(2):83-93. doi: 10.1016/j.dental.2003.12.002.
To evaluate the effect of increasing the dentin conditioning time with self-etching primers of different aggressiveness (pH) on the microtensile bond strength (muTBS) of three resin cements.
Pre-cured composite blocks were cemented with M-Bond, Bistite II DC, or Panavia F to flat occlusal dentin surfaces of human third molars, which were conditioned with M-Bond or Bistite II-primer for 30, 60 or 180 s or with Panavia-primer for 60 or 180 s. Each dentin-composite block assembly (four in each group) was longitudinally sectioned to obtain 1x1 mm microbars and tested for the muTBS. The morphology of the conditioned dentin surface and the hybrid layer was examined with SEM.
Extending the primer conditioning time for Bistite II DC from 30 to 60 s significantly increased the muTBS (p<0.001) but did not further increase from 60 s to 180 s. For M-Bond there was only a significant increase from 30 to 180 s (p<0.05). For Panavia F the primer-conditioning time had no influence on the muTBS. SEM observations of conditioned dentin showed that the Bistite II DC and M-Bond self-etching primers with the lowest pH completely dissolved the dentin smear layer and plugs and formed well-defined hybrid layers. This was not found for Panavia F.
Dentin bond strength of resin cements using more aggressive self-etching primers is improved by increasing the conditioning time. To enable resin infiltration of highly filled resin cements, sufficient smear layer dissolution is necessary.
评估使用不同侵蚀性(pH值)的自酸蚀底漆延长牙本质预处理时间对三种树脂水门汀微拉伸粘结强度(μTBS)的影响。
将预固化的复合树脂块用M-Bond、Bistite II DC或Panavia F粘结到人第三磨牙平坦的咬合面牙本质表面,这些牙本质表面分别用M-Bond或Bistite II底漆预处理30、60或180秒,或用Panavia底漆预处理60或180秒。将每个牙本质-复合树脂块组件(每组四个)纵向切片以获得1×1毫米的微条,并测试其μTBS。用扫描电子显微镜(SEM)检查预处理后的牙本质表面和混合层的形态。
将Bistite II DC的底漆预处理时间从30秒延长至60秒可显著提高μTBS(p<0.001),但从60秒延长至180秒时未进一步提高。对于M-Bond,仅从30秒至180秒有显著提高(p<0.05)。对于Panavia F,底漆预处理时间对μTBS没有影响。预处理牙本质的SEM观察表明,pH值最低的Bistite II DC和M-Bond自酸蚀底漆完全溶解了牙本质玷污层和牙本质小管堵塞物,并形成了清晰的混合层。Panavia F则未出现这种情况。
使用侵蚀性更强的自酸蚀底漆时,延长预处理时间可提高树脂水门汀与牙本质的粘结强度。为使高填料树脂水门汀能够渗入,充分溶解玷污层是必要的。