Gaintantzopoulou Marianna, Kakaboura Afrodite, Vougiouklakis Georgios
Eur J Prosthodont Restor Dent. 2005 Jun;13(2):51-6.
The colour stability of the surface and in-depth (2 mm) layer of two resin composites, a laboratory second-generation resin composite and a compomer were evaluated after 24 and 360 hours of water aging under dark and UV light conditions. The influence of various polymerization techniques on color changes was also evaluated. Color differences (deltaE*) showed higher color changes under UV light exposure than under dark storage, both at 24- and 360-hour evaluations. Color changes were statistically higher at the 360-hour assessment, in both conditions of maintenance. Compomer was the least color stable of the materials tested. Additional polymerization significantly decreased the colour change of both composite resins.
在黑暗和紫外线条件下进行24小时和360小时水老化后,评估了两种树脂复合材料(一种实验室第二代树脂复合材料和一种复合体)表面及深度(2毫米)层的颜色稳定性。还评估了各种聚合技术对颜色变化的影响。在24小时和360小时的评估中,色差(ΔE*)显示在紫外线照射下的颜色变化高于黑暗储存条件下。在两种保存条件下,360小时评估时的颜色变化在统计学上更高。复合体是测试材料中颜色稳定性最差的。额外聚合显著降低了两种复合树脂的颜色变化。