Malekipour Mohammad Reza, Sharafi Ala, Kazemi Shantia, Khazaei Saber, Shirani Farzaneh
Department of Operative Dentistry, Faculty of Dentistry, Azad University, Khorasgan (Isfahan Branch), Isfahan, Iran.
Dent Res J (Isfahan). 2012 Jul;9(4):441-6.
Color change of composite restorations in different color media during the time is a common problem in esthetic dentistry, causing the need to replace the restoration, and spending a great deal of cost and time to patients. The aim of this study is to investigate the effects of different common drinks consumed by patients on one of the widely used composites in dentistry.
Sixty-five disk-shaped specimens were prepared with a light-cured composite (Z100-shade A2) and divided into five groups of 13 specimens. Samples of each group were immersed in staining solutions (tea, coffee, lemonade, and cola) and distilled water (as control). Color values (L*, a*, b*) were measured relative to the standard illuminant D65 over a white background, using the CIE Lab* system. Color change values were calculated before and after 1, 7, and 14 days of immersion. Repeated measures and one-way analysis of variance (ANOVA) and paired t tests were applied for statistical analysis.
Tea and coffee produced the most discoloration, whereas, water exhibited the least color change after immersion for 14 days in Z100 (P < 0.05). After one day of immersion, coffee caused the lowest discoloration in the test composite, compared to tea, cola, distilled water, and lemonade (P < 0.05).
Staining solutions and immersion time are significant factors that affect color stability of composite resins.
在美学牙科领域,复合树脂修复体在不同颜色介质中随时间发生颜色变化是一个常见问题,这导致需要更换修复体,给患者带来大量成本和时间消耗。本研究的目的是调查患者饮用的不同常见饮品对牙科广泛使用的一种复合材料的影响。
用光固化复合材料(Z100-A2色)制备65个圆盘形标本,并分为五组,每组13个标本。每组样本浸入染色溶液(茶、咖啡、柠檬水和可乐)和蒸馏水(作为对照)中。使用CIE Lab系统,在白色背景下相对于标准照明体D65测量颜色值(L、a*、b*)。在浸泡1天、7天和14天后计算颜色变化值。采用重复测量和单因素方差分析(ANOVA)以及配对t检验进行统计分析。
在Z100中浸泡14天后,茶和咖啡导致的变色最多,而水的颜色变化最小(P < 0.05)。浸泡一天后,与茶、可乐、蒸馏水和柠檬水相比,咖啡导致测试复合材料的变色最低(P < 0.05)。
染色溶液和浸泡时间是影响复合树脂颜色稳定性的重要因素。