Abstract

STATEMENT OF PROBLEM

The color instability and degradation of maxillofacial elastomers limit the function and cosmetic quality of facial prostheses.

PURPOSE

The purpose of this study was to measure the interactions of oil pigments plus dry earth opacifiers at 5%, 10%, and 15% by volume in stabilizing the color of MDX4-4210/type A silicone elastomers before and after artificial aging.

MATERIAL AND METHODS

In the first part of the study, each of 5 opacifiers (Georgia kaolin powder neutral, kaolin powder calcined, Artskin white, dry pigment titanium (Ti) white, or Ti white artists' oil color) at 10% concentrations were combined with each of 5 oil pigment types (no pigment, cadmium-barium red deep, yellow ochre, burnt sienna, or a mixture of the 3 pigments), for a total of 25 experimental groups of elastomers. In the second part of the study, 50 experimental groups of elastomers were made by combining 1 of 5 opacifiers at 5% and 15% concentrations with 1 of 5 oil pigments as in Part 1. Five specimens of each elastomer were tested, for a total of 375 specimens. In each part of the study, all specimens were aged in an artificial aging chamber. CIE Lab* values were measured by a spectrophotometer. The color differences (DeltaE*) were subjected to repeated-measures analysis of variance. Mean values were compared by Tukey-Kramer intervals (alpha = .05).

RESULTS

In Part 1, when the opacifiers were tested at 10% concentration, Ti white oil color had the most color change, and dry pigment Ti white had the least; all other opacifiers were not significantly different from each other. In Part 2, at 5%, Ti white oil color had the most color change; all other opacifiers were not significantly different from the others. At 15%, Ti white oil color again had the most color change, followed by Artskin white, kaolin powder calcined, and Georgia kaolin; Ti white dry earth pigment had the least color change. Overall, 5% Artskin white had less color change than the 15%, whereas 15% dry pigment Ti white had less color change than the 5% (P < .001). The 5% and 15% of other opacifiers were not significantly different.

CONCLUSIONS

At all 3 concentrations, oil pigments mixed with opacifiers helped protect the MDX4-4210/type A silicone elastomer from color degradation over time. Dry pigment Ti white remained the most color stable over time, followed by the pigments mixed with kaolin powder calcined, Georgia kaolin, Artskin white, and Ti white artists' oil color.

摘要

问题陈述

颌面弹性体的颜色不稳定性和降解限制了面部假体的功能和美观质量。

目的

本研究的目的是测量体积分数为5%、10%和15%的油性颜料加干土遮光剂在人工老化前后对MDX4-4210/A型硅橡胶弹性体颜色的稳定作用。

材料与方法

在研究的第一部分,将5种遮光剂(中性佐治亚高岭土粉、煅烧高岭土粉、Artskin白色、干颜料钛白或钛白艺术家油彩)各以10%的浓度与5种油性颜料类型(无颜料、镉钡深红、赭石黄、焦赭石或这3种颜料的混合物)中的每种进行组合,共得到25个弹性体实验组。在研究的第二部分,如第一部分那样,将5种遮光剂中浓度为5%和15%的1种与5种油性颜料中的1种进行组合,制成50个弹性体实验组。对每种弹性体的5个样本进行测试,共375个样本。在研究的每个部分,所有样本都在人工老化箱中老化。用分光光度计测量CIE Lab值。对颜色差异(ΔE)进行重复测量方差分析。均值通过Tukey-Kramer区间进行比较(α = 0.05)。

结果

在第一部分中,当遮光剂以10%的浓度进行测试时,钛白艺术家油彩的颜色变化最大,干颜料钛白的颜色变化最小;所有其他遮光剂之间没有显著差异。在第二部分中,在5%时,钛白艺术家油彩的颜色变化最大;所有其他遮光剂之间没有显著差异。在15%时,钛白艺术家油彩的颜色变化仍然最大,其次是Artskin白色、煅烧高岭土粉和佐治亚高岭土;干土颜料钛白的颜色变化最小。总体而言,5%的Artskin白色的颜色变化小于15%的;而15%的干颜料钛白的颜色变化小于5%的(P < 0.001)。其他遮光剂的5%和15%之间没有显著差异。

结论

在所有3种浓度下,油性颜料与遮光剂混合有助于保护MDX4-4210/A型硅橡胶弹性体随时间推移不发生颜色降解。干颜料钛白随时间推移颜色稳定性仍然最高,其次是与煅烧高岭土粉、佐治亚高岭土、Artskin白色和钛白艺术家油彩混合的颜料。