Savina Irina N, Galaev Igor Yu, Mattiasson Bo
Department of Biotechnology, Center for Chemistry and Chemical Engineering, Lund University, SE-22100 Lund, Sweden.
J Mol Recognit. 2006 Jul-Aug;19(4):313-21. doi: 10.1002/jmr.774.
The grafting of functional polymers to the pore surface of macroporous monolithic polyacrylamide cryogels was found to be an efficient and convenient method for the preparation of macroporous polyacrylamide gels, so-called cryogels (pAAm cryogels), with both controlled extent of functional group incorporated and with tailored surface chemistries. Anion-exchange polymer chains of poly(2-(dimethylamino)ethyl methacrylate) (pDMAEMA) and poly([2-(methacryloyloxy)ethyl]-trimethylammonium chloride) (pMETA), and cation-exchange polymer chains of polyacrylate have been grafted onto pAAm cryogels using potassium diperiodatocuprate as initiator. It was possible to achieve the ion-exchange capacity up to 0.2-0.5 mmol/ml. The graft polymerization did not alter the macroporous structure of the pAAm cryogel, however the flow rate of solutes through the cryogel matrix decreased with increase in the density of polymer grafted. The sorption of low-molecular-weight (metal ion, dye) and high-molecular-weight (protein) substances on the grafted monolithic pAAm column has been studied. The results indicate that a 'tentacle'-type binding of protein to grafted polymer depended on the architecture of the grafted polymer layer and took place after a certain degree of grafting has been reached. The binding of proteins by tentacle-like polymer chains allowed for increasing the binding capacity for proteins on the grafted pAAm cryogels up to 6-12 mg/ml.
将功能聚合物接枝到大孔整体聚丙烯酰胺冷冻凝胶的孔表面,被发现是制备大孔聚丙烯酰胺凝胶(即所谓的冷冻凝胶,pAAm冷冻凝胶)的一种有效且便捷的方法,这种方法能够控制官能团的引入程度并定制表面化学性质。以二高碘酸铜钾为引发剂,将聚(甲基丙烯酸2-(二甲氨基)乙酯)(pDMAEMA)和聚([2-(甲基丙烯酰氧基)乙基]三甲基氯化铵)(pMETA)的阴离子交换聚合物链以及聚丙烯酸的阳离子交换聚合物链接枝到pAAm冷冻凝胶上。离子交换容量可达0.2 - 0.5 mmol/ml。接枝聚合并未改变pAAm冷冻凝胶的大孔结构,然而,随着接枝聚合物密度的增加,溶质通过冷冻凝胶基质的流速降低。研究了低分子量(金属离子、染料)和高分子量(蛋白质)物质在接枝的整体pAAm柱上的吸附情况。结果表明蛋白质与接枝聚合物的“触手”型结合取决于接枝聚合物层的结构,且在达到一定接枝程度后发生。触手状聚合物链对蛋白质的结合使得接枝的pAAm冷冻凝胶对蛋白质的结合容量提高到6 - 12 mg/ml。