人成骨细胞对含羟基磷灰石和二氧化钛成分的溶胶-凝胶改性钛的初始反应。

Initial responses of human osteoblasts to sol-gel modified titanium with hydroxyapatite and titania composition.

作者信息

Harle Jamie, Kim Hae-Won, Mordan Nicky, Knowles Jonathan C, Salih Vehid

机构信息

Division of Biomaterials and Tissue Engineering, Eastman Dental Institute, University College London, 256 Gray's Inn Road, London WC1X 8LD, UK.

出版信息

Acta Biomater. 2006 Sep;2(5):547-56. doi: 10.1016/j.actbio.2006.05.005. Epub 2006 Jul 10.

Abstract

Sol-gel thin films of hydroxyapatite (HA) and titania (TiO(2)) have received a great deal of attention in the area of bioactive surface modification of titanium (Ti) implants. Sol-gel coatings were developed on Ti substrates of pure HA and TiO(2) and two composite forms, HA+10% TiO(2) and HA+20% TiO(2), and the biological properties of the coatings were evaluated. All the coating layers exhibited thin and homogeneous structures and phase-pure compositions (either HA or TiO(2)). Primary human osteoblast cells showed good attachment, spreading and proliferation on all the sol-gel coated surfaces, with enhanced cell numbers on all the coated surfaces relative to uncoated Ti control at day 1, as observed by MTT assay and scanning electron microscopy. Cell attachment rates were also enhanced on the pure HA coating relative to control Ti. The pure HA and HA+10% TiO(2) composite coating furthermore enhanced proliferation of osteoblasts at 4 days. Moreover, the gene expression level of several osteogenic markers including bone sialoprotein and osteopontin, as measured by RT-PCR at 24h, was shown to vary according to coating composition. These findings suggest that human primary bone cells show marked and rapid early functional changes in response to HA and TiO(2) sol-gel coatings on Ti.

摘要

羟基磷灰石(HA)和二氧化钛(TiO₂)的溶胶 - 凝胶薄膜在钛(Ti)植入物的生物活性表面改性领域受到了广泛关注。在纯HA、TiO₂以及两种复合形式(HA + 10% TiO₂和HA + 20% TiO₂)的Ti基底上制备了溶胶 - 凝胶涂层,并对涂层的生物学性能进行了评估。所有涂层均呈现出薄且均匀的结构以及纯相组成(HA或TiO₂)。原代人成骨细胞在所有溶胶 - 凝胶涂层表面均表现出良好的附着、铺展和增殖,通过MTT法和扫描电子显微镜观察发现,在第1天时,相对于未涂层的Ti对照,所有涂层表面的细胞数量均有所增加。相对于对照Ti,纯HA涂层上的细胞附着率也有所提高。此外,纯HA和HA + 10% TiO₂复合涂层在4天时进一步促进了成骨细胞的增殖。而且,通过RT - PCR在24小时测量发现,包括骨唾液蛋白和骨桥蛋白在内的几种成骨标志物的基因表达水平会因涂层组成而有所不同。这些发现表明,人原代骨细胞对Ti上的HA和TiO₂溶胶 - 凝胶涂层会表现出显著且快速的早期功能变化。