Zhang Yu Xi, Wu Fei Peng, Li Miao Zhen, Wang Er Jian
Technical Institute of Physics and Chemistry, Chinese Academy of Sciences, Beijing 100101, China.
J Phys Chem B. 2005 Dec 1;109(47):22250-5. doi: 10.1021/jp054315i.
Hydrophobically associating copolymers of acrylamide (AM) with a small amount of 4-(omega-propenoyloxyethoxy) benzoic acid (PEBA, <2.5%) were synthesized by template copolymerization in the presence of poly(allylammonium chloride) (PAAC) as a template in an aqueous medium. These template copolymers exhibited remarkable thickening properties due to the effective hydrophobic association, which were similar to those copolymers with a multiblock structure obtained by the micellar process. The pH of the reaction medium and the molecular weight of the template strongly influenced the thickening properties of the products. In the experimental range, the higher the PEBA content, the larger the thickening capacity of these hydrophobic copolymers. The aggregate behaviors of these copolymers were studied by fluorescence, transmission electron microscopy (TEM), and light scattering techniques. The apparent critical interpolymer aggregate concentration (cac) of the copolymer solution was about 0.5 g/dL. As the concentration of the copolymer became higher than the cac, the aggregates changed their morphology from small hollow spheres to big flower-shaped aggregates. All the above results indicated that the template copolymerization gave access to a very simple and powerful means for the preparation of hydrophobically associating copolymers and other functional polymer materials.
以聚烯丙基氯化铵(PAAC)为模板,在水介质中通过模板共聚法合成了丙烯酰胺(AM)与少量4 - (ω - 丙烯酰氧基乙氧基)苯甲酸(PEBA,<2.5%)的疏水缔合共聚物。由于有效的疏水缔合作用,这些模板共聚物表现出显著的增稠性能,这与通过胶束法获得的具有多嵌段结构的共聚物相似。反应介质的pH值和模板的分子量对产物的增稠性能有强烈影响。在实验范围内,PEBA含量越高,这些疏水共聚物的增稠能力越大。通过荧光、透射电子显微镜(TEM)和光散射技术研究了这些共聚物的聚集行为。共聚物溶液的表观临界聚合物间聚集浓度(cac)约为0.5 g/dL。当共聚物浓度高于cac时,聚集体的形态从小空心球变为大花状聚集体。上述所有结果表明,模板共聚为制备疏水缔合共聚物和其他功能高分子材料提供了一种非常简单而有效的方法。