Suppr超能文献

完整牙本质和龋损牙本质粘结-牙本质界面耐酸碱区的形态学和力学特性

Morphological and mechanical characterization of the acid-base resistant zone at the adhesive-dentin interface of intact and caries-affected dentin.

作者信息

Inoue Go, Tsuchiya Satoko, Nikaido Toru, Foxton Richard M, Tagami Junji

机构信息

Cariology and Operative Dentistry, Department of Restorative Sciences, Graduate School, Tokyo Medical and Dental University, Japan.

出版信息

Oper Dent. 2006 Jul-Aug;31(4):466-72. doi: 10.2341/05-62.

Abstract

This study examined the ultrastructure of both intact and caries affected dentin-adhesive interface after artificial secondary caries formation, using scanning electron microscopy and nanoindentation testing. Half of the prepared specimens were bonded with Clearfil SE Bond (Kuraray Medical, Japan) and a resin composite (Metafil Flo, Sun Medical, Japan) for the nanoindentation test. The other specimens were stored in a buffered demineralizing solution for 90 minutes, then observed using SEM. An acid-base resistant zone (ABRZ) was observed beneath the hybrid layer, distinguished by argon-ion etching. The ABRZ of caries-affected dentin was thicker than that of normal dentin, while its nanohardess was lower than normal dentin (p<0.05). It is suggested that the monomer of Clearfil SE Bond penetrated deeper than previously reported, creating a so-called "hybrid layer." However, its physical properties depended on the condition of the dentin.

摘要

本研究采用扫描电子显微镜和纳米压痕测试,观察了人工继发龋形成后完整牙本质与龋损牙本质-粘结界面的超微结构。制备的标本一半用Clearfil SE Bond(日本可乐丽医疗株式会社)和树脂复合材料(日本太阳医疗株式会社的Metafil Flo)粘结,用于纳米压痕测试。另一半标本在缓冲脱矿溶液中保存90分钟,然后用扫描电子显微镜观察。通过氩离子蚀刻在混合层下方观察到一个耐酸碱区(ABRZ)。龋损牙本质的ABRZ比正常牙本质厚,但其纳米硬度低于正常牙本质(p<0.05)。提示Clearfil SE Bond的单体渗透深度比先前报道的更深,形成了所谓的“混合层”。然而,其物理性能取决于牙本质的状况。