[牙科常用修复合金瞬间电流强度的测定]

[Measuration of instantly galvanic current magnitude among dental common restorative alloys].

作者信息

Cao Yan-Lan, Zhu Song, Shan Yi-Bin

机构信息

Dept. of Prosthetics, College of Stomatology, Jilin University, Changchun 1030041, China.

出版信息

Hua Xi Kou Qiang Yi Xue Za Zhi. 2006 Dec;24(6):516-9.

Abstract

OBJECTIVE

To measure the magnitude of galvanic currents produced by different occluding metallic contact.

METHODS

The circuits of instantly different metallic contact were simulated in artificial saliva, and electrical potential of every couple and 15 currents of instant contact were then measured. After 8 hours' soaking, 15 currents were obtained in addition.

RESULTS

Galvanic currents variation produced hy intermittently metallic contact was ruleless. During early soaking, gold/titanium, gold/high zinc-containing amalgam and low/high zinc-containing amalgam exhibited much higher current, and there was significant difference on currents between titanium/high zinc-containing amalgam and other couples (P < 0.05). There was also significant difference on currents between titanium/high zinc containing amalgam, titanium/low zinc-containing amalgam and gold/titanium, gold/low zinc-containing amalgam and gold/high zinc-containing amalgam after 8 hours' soaking (P < 0.05). In contrast with currents produced by couples before and after 8 hours' soaking, only the currents produced by gold/high zinc-containing amalgam proved to be no significant of difference (P > 0.05), while the currents produced by gold/low zinc-containing amalgam and titanium/high zinc-containing amalgam increased. Potential of high zinc-containing amalgam was more negative than other alloys, and it was always under anodic behavior during the experiment corrupted acceleratedly.

CONCLUSION

Dentists can't ignore the case that the patient feels normal at the beginning of wearing different occluding metallic restorations. Either of gold/ titatium, gold/high zinc-containing amalgam and low/high zinc-containing amalgam appearing in oral will do harm to the patients' health. Neither of gold/low zinc-containing amalgam nor titanium/high zinc-containing amalgam can coexist in oral. Zinc-free or low zinc-containing amalgam should be selected instead of high zinc-containing amalgam.

摘要

目的

测量不同咬合金属接触产生的电流强度。

方法

在人工唾液中模拟即时不同金属接触的电路,然后测量每对的电位和15次即时接触的电流。浸泡8小时后,又获得了15次电流。

结果

间歇性金属接触产生的电流变化无规律。在浸泡初期,金/钛、金/高锌汞合金和低/高锌汞合金表现出更高的电流,钛/高锌汞合金与其他配对之间的电流存在显著差异(P<0.05)。浸泡8小时后,钛/高锌汞合金、钛/低锌汞合金与金/钛、金/低锌汞合金和金/高锌汞合金之间的电流也存在显著差异(P<0.05)。与浸泡8小时前后配对产生的电流相比,只有金/高锌汞合金产生的电流差异无统计学意义(P>0.05),而金/低锌汞合金和钛/高锌汞合金产生的电流增加。高锌汞合金的电位比其他合金更负,在实验过程中始终处于阳极行为,腐蚀加速。

结论

牙医不能忽视患者在佩戴不同咬合金属修复体初期感觉正常的情况。口腔中出现的金/钛、金/高锌汞合金和低/高锌汞合金中的任何一种都会对患者健康造成损害。金/低锌汞合金和钛/高锌汞合金都不能在口腔中共存。应选择无锌或低锌汞合金而非高锌汞合金。