Clin Oral Implants Res. 2007 Apr;18(2):153-60. doi: 10.1111/j.1600-0501.2006.01316.x.

Abstract

The texture of an implant's surface can influence the rate and extent of bone fixation as expressed by the amount of linear bone-to-implant contact (BIC). The purpose of this study was to compare the bone density and linear BIC between Osseotite and machined-surface implants placed in bony defects without graft material and covered by a membrane. Thirty 2 mm diameter, 10 mm length custom implants were prepared for this study having a 'split surface,' with one side having the acid-etched surface and the opposite side having a machined surface. Defects were created in the iliac wing of three adult mongrel dogs where a 6-mm-diameter drill was used to generate a 5-mm-deep defect. The implants were inserted into the center of the defect with 5 mm secured into the bone leaving 5 mm free in the defect with a 2 mm gap between the implant and surrounding bone. Expanded polytetrafluroethelyene membranes were placed over the defect sites stabilized with Biotack pins. The healing times were 2, 3, and 5 months. Histologic and histometric analysis showed significantly lower BIC in the defect region as compared with the portion of implant placed into native bone for both implant surfaces in all groups. There was no difference in BIC values at 2- and 5-month periods between the two surfaces in the regenerated area, while BIC values for Osseotite surfaces were significantly higher than the machined surfaces at 3 months' healing time. Changes in bone density, observed between the three groups, affected correspondingly the BIC values in both implant surfaces, the effect being more pronounced in the Osseotite surface.

摘要

种植体表面的质地可影响骨固定的速率和程度,这可通过线性骨与种植体接触(BIC)的量来体现。本研究的目的是比较在未使用移植材料且覆盖有膜的骨缺损处植入的Osseotite种植体和机械加工表面种植体之间的骨密度和线性BIC。为该研究制备了30枚直径2mm、长度10mm的定制种植体,其具有“分裂表面”,一侧为酸蚀表面,另一侧为机械加工表面。在三只成年杂种犬的髂骨翼制造缺损,使用直径6mm的钻头制造5mm深的缺损。将种植体插入缺损中心,5mm固定于骨内,缺损内留5mm,种植体与周围骨之间有2mm间隙。用生物钉将膨体聚四氟乙烯膜置于缺损部位。愈合时间分别为2个月、3个月和5个月。组织学和组织计量学分析显示,在所有组中,与植入天然骨的种植体部分相比,缺损区域的BIC显著更低。在再生区域,两个表面在2个月和5个月时的BIC值无差异,而在愈合3个月时,Osseotite表面的BIC值显著高于机械加工表面。三组之间观察到的骨密度变化相应地影响了两个种植体表面的BIC值,这种影响在Osseotite表面更为明显。