Suppr超能文献

两种不同黏接系统释放的 HEMA 的高效液相色谱分析。

HPLC analysis of HEMA released from two different adhesive systems.

机构信息

Department of Prosthodontics, Karadeniz Technical University, Trabzon, Turkey.

Department of Prosthodontics, School of Dentistry, Gaziantep University, Gaziantep, Turkey.

出版信息

J Biomed Mater Res B Appl Biomater. 2009 Nov;91(2):924-929. doi: 10.1002/jbm.b.31476.

Abstract

OBJECTIVES

The aim of this study was to evaluate in vitro elution of 2-Hydroxyethyl methacrylate (HEMA) from two different adhesive systems, used in two dual polymerized resin cements for bonding of ceramic restoration by high performance liquid chromatography (HPLC).

METHODS

Twenty freshly extracted caries and restoration free molar teeth used in this study. Standardized Class I preparations were prepared in all teeth. A lithium disilicate based (IPS Empress Esthetic; Ivoclar) ceramic inlays were cemented with one of the dual polymerized resin cements (RelyX ARC; 3M ESPE or Nexus 2; Kerr) that have two different adhesive systems (Single Bond; 3M ESPE, Optibond Solo Plus; Kerr). After cementation, specimens were stored in 75% ethanol solution. HPLC was used to analyze the amount of HEMA in the solution (after 10 min, 1 h, 24 h, 3, 7, 14, and 21 days). Two-way analysis of variance and Tukey HSD tests were used to evaluate the results (p < 0.05).

RESULTS

There were statistically significant differences between adhesive systems according to the amount of released HEMA (p < 0.01) and also among time periods (p < 0.01). The amount of HEMA eluted from Optibond Solo Plus was significantly higher than Single Bond. The total amount of monomers was the highest after 21 days (p < 0.01).

CONCLUSIONS

In the case of adhesive systems, Optibond Solo Plus showed the highest amount of HEMA. The amount of HEMA eluted from adhesive systems influenced by the time.

摘要

目的

本研究旨在通过高效液相色谱法(HPLC)评估两种不同的黏接系统从两种用于双重聚合树脂黏结陶瓷修复体的树脂黏结剂中洗脱 2-羟乙基甲基丙烯酸酯(HEMA)的体外洗脱情况。

方法

本研究共使用了 20 颗刚从患者口腔中拔出的、无龋坏和修复体的磨牙。所有牙齿均制备了标准化的 I 类备洞。将一种基于锂二硅的(IPS Empress Esthetic;Ivoclar)陶瓷嵌体用两种不同黏接系统(Single Bond;3M ESPE,Optibond Solo Plus;Kerr)的其中一种双重聚合树脂黏结剂(RelyX ARC;3M ESPE 或 Nexus 2;Kerr)黏结。黏结后,将样本储存在 75%乙醇溶液中。HPLC 用于分析溶液中 HEMA 的含量(10 分钟、1 小时、24 小时、3 天、7 天、14 天和 21 天后)。采用双因素方差分析和 Tukey HSD 检验进行数据分析(p < 0.05)。

结果

根据释放的 HEMA 量(p < 0.01)和时间周期(p < 0.01),黏接系统之间存在显著差异。Optibond Solo Plus 洗脱的 HEMA 量明显高于 Single Bond。21 天后单体总量最高(p < 0.01)。

结论

在黏接系统方面,Optibond Solo Plus 显示出最高的 HEMA 量。黏接系统中洗脱的 HEMA 量受时间影响。