Altunsoy Mustafa, Selim Botsali Murat, Ulker Hayriye Esra
Department of Pediatric Dentistry, Faculty of Dentistry, Sifa University, Izmir - Turkey.
Department of Pediatric Dentistry, Faculty of Dentistry, Selcuk University, Konya - Turkey.
J Appl Biomater Funct Mater. 2015 Jul 4;13(2):e100-5. doi: 10.5301/jabfm.5000200.
This study evaluated the elution of 2-hydroxyethyl methacrylate (HEMA) from 4 different adhesives, using high-performance liquid chromatography (HPLC).
The adhesives were applied on a bovine dentin surface and polymerized using an LED curing unit (n=5). After polymerization, specimens were stored in 75% ethanol solution (6 mL). Residual HEMA that was eluted from adhesives (after 10 minutes, 1 hour, 24 hours, 7 days and 30 days) was analyzed using HPLC. Statistical analyses were performed using 1-way ANOVA, Tukey HSD test and paired 2-sample t-test.
There were statistically significant differences among adhesive systems for the cumulative released HEMA and among the time periods (p<0.05). Clearfil SE Bond showed the highest amount of HEMA released, while Easy Bond showed the lowest. Among the time periods, the highest eluted HEMA value was detected in 10 minutes for all adhesives, and elution continued for up to 30 days.
The HEMA eluted from adhesives was in different amounts, and the elution continued for a long time. The amount of eluted HEMA from adhesives used in this study was not viewed as critical for toxic reactions in biological tissues.
本研究采用高效液相色谱法(HPLC)评估了4种不同黏结剂中甲基丙烯酸羟乙酯(HEMA)的洗脱情况。
将黏结剂涂覆于牛牙本质表面,并用发光二极管固化装置进行聚合(n = 5)。聚合后,将标本置于75%乙醇溶液(6 mL)中。使用HPLC分析从黏结剂中洗脱出来的残留HEMA(在10分钟、1小时、24小时、7天和30天后)。采用单因素方差分析、Tukey HSD检验和配对双样本t检验进行统计分析。
对于累积释放的HEMA,不同黏结剂系统之间以及不同时间段之间存在统计学显著差异(p<0.05)。Clearfil SE Bond释放的HEMA量最高,而Easy Bond释放的量最低。在所有时间段中,所有黏结剂在10分钟时检测到的HEMA洗脱值最高,且洗脱持续长达30天。
从黏结剂中洗脱的HEMA量各不相同,且洗脱会持续很长时间。本研究中使用的黏结剂洗脱的HEMA量在生物组织的毒性反应方面不被视为关键因素。