Yap Y K, Inagaki M, Nakajima S, Mori Y, Sasaki T
Opt Lett. 1996 Sep 1;21(17):1348-50. doi: 10.1364/ol.21.001348.
High pulse energies of nanosecond-level fourth- and fifth-harmonic (4omega and 5omega) generation of a Nd:YAG laser have been obtained with a CsLiB(6)O(10) (CLBO) nonlinear crystal. 500 mJ of 4omega output with a conversion efficiency of 50% from the second-harmonic input was generated. 5omega output at 213 nm of as high as 230 mJ was obtained by sum-frequency generation of the 266- and 1064-nm beams, corresponding to a 10.4% conversion efficiency of the initial fundamental input energy. The characteristics of the CLBO crystal that permit this effective frequency conversion are discussed.