PURPOSE

To determine the in vitro dentinal fluid movement produced by various osmotic stimuli, and evaluate fluid movement across human dentin in response to the application of various osmotic stimuli before and after the application of self-etching adhesive (Clearfil S3 Bond).

MATERIALS AND METHODS

The experiments were carried out on 10 extracted premolars. Each tooth was cut transversely below to the cementoenamel junction with a diamond disk and water coolant. Dentin was exposed at the tip of the buccal cusp by cutting a cavity and was etched with acid. The osmotic stimuli were solutions of saturated CaCl2, sugar syrup, chocolate, and sweet Thai dessert, used as osmotic test solutions, randomly applied to dentin.The fluid flow through dentin obtained after 15 s of application of each osmotic stimulus was measured before and after bonding with Clearfil S3 Bond single-dose.

RESULTS

Before bonding procedures, CaCl2 produced peak rates of fluid flow that were significantly higher (p <0.001), when compared with normal saline, sugar syrup, chocolate, and sweet Thai dessert. During the applications of all osmotic stimuli, the amount of fluid movement across resin-bonded dentin was significantly lower than that without adhesives. There were no significant differences of fluid shifts across resin-bonded dentin obtained during the application of any osmotic stimuli.

CONCLUSION

It appears that different osmotic stimuli produced different rates of outward fluid flow through dentin. Clearfil S3 Bond produced similar significant reductions of fluid movement in response to osmotic stimulation, irrespective of the chemical composition, or the osmotic pressure of stimuli.

摘要

目的

确定不同渗透刺激物产生的体外牙本质液流,并评估在应用自酸蚀粘结剂(Clearfil S3 Bond)前后,各种渗透刺激物作用于牙本质时牙本质内液流的移动。

材料和方法

在 10 颗离体前磨牙上进行了实验。每颗牙齿均用金刚石片和水冷却剂在釉牙骨质界以下横断切开。通过在颊尖处切一洞并用酸蚀刻暴露牙本质。用饱和 CaCl2 溶液、糖浆、巧克力和甜泰式甜点溶液作为渗透测试溶液,随机应用于牙本质,测试液在 15 s 渗透牙本质后,测量其流动。在应用 Clearfil S3 Bond 单剂量粘结前和粘结后,测量每种渗透刺激物作用后的牙本质液流。

结果

在粘结程序之前,与生理盐水、糖浆、巧克力和甜泰式甜点相比,CaCl2 产生的峰值牙本质液流速率显著更高(p <0.001)。在所有渗透刺激物应用过程中,粘结剂处理过的牙本质内的液体移动量明显低于无粘结剂的牙本质。应用任何渗透刺激物时,在粘结剂处理过的牙本质内的液体移动量没有显著差异。

结论

不同的渗透刺激物似乎产生了不同的牙本质外向液流速率。Clearfil S3 Bond 对渗透刺激产生了类似的显著减少牙本质液流的效果,而与刺激物的化学成分或渗透压无关。