J Endod. 2010 Mar;36(3):493-6. doi: 10.1016/j.joen.2009.11.009. Epub 2010 Jan 25.
Retreatment procedures might affect the adhesion capability of refilling materials to dentinal walls. The purpose of this study was to compare the effect of different retreatment techniques on bond strength of Resilon (Resilon Research LLC, Madison, CT)/Epiphany (Pentron Clinical Technologies, LLC, Wallingford, CT) self-etch (SE) with radicular dentin after canal reobturation.
Sixty extracted single-rooted human teeth were prepared using Mtwo rotary files (VDW, Munich, Germany) and obturated with Resilon/Epiphany SE. The roots were randomly divided into four groups; in group 1, no retreatment procedure was done; group 2 was retreated using Mtwo R/Mtwo files; group 3 was retreated using Mtwo R/Mtwo combined with chloroform; and group 4 was retreated using Mtwo R/Mtwo combined with Endosolv R (Septodont, Paris, France). The root canals were then reobturated with Resilon/Epiphany SE. One-millimeter slices of midroot dentin were prepared for the push-out test (n=30 slices per group). Failure modes after the push-out test were examined under microscopy. The data were analyzed by using a one-way analysis of variance and the Dunnett post hoc test.
Group 3 showed significantly the lowest mean bond strength (p<0.02). No significant difference was found between the values of groups 1, 2, and 4 (p>0.26). The mode of bond failure was predominantly adhesive for all groups.
This study showed that the bond strength of Resilon/Epiphany SE after root canal retreatment using Mtwo files, either alone or combined with Endosolv R, was not significantly different from that of nonretreated specimens. Chloroform used for retreatment had an adverse effect on the bond strength of Resilon/Epiphany SE after root canal reobturation.
再治疗程序可能会影响填充材料对牙本质壁的附着力。本研究的目的是比较不同再治疗技术对根管再填充后牙本质的 Resilon(Resilon Research LLC,Madison,CT)/Epiphany(Pentron Clinical Technologies,LLC,Wallingford,CT)自酸蚀(SE)黏结强度的影响。
60 颗单根人牙使用 Mtwo 旋转锉(VDW,慕尼黑,德国)进行预备,并使用 Resilon/Epiphany SE 进行根管填充。将牙根随机分为四组;在第 1 组中,不进行再治疗;第 2 组使用 Mtwo R/Mtwo 锉进行再治疗;第 3 组使用 Mtwo R/Mtwo 联合氯仿进行再治疗;第 4 组使用 Mtwo R/Mtwo 联合 Endosolv R(Septodont,巴黎,法国)进行再治疗。然后使用 Resilon/Epiphany SE 重新填充根管。制备中根牙 1mm 切片进行推出试验(每组 30 个切片)。在显微镜下检查推出试验后的失效模式。使用单向方差分析和 Dunnett 事后检验对数据进行分析。
第 3 组的平均黏结强度最低(p<0.02)。第 1、2 和 4 组之间的数值无显著差异(p>0.26)。所有组的黏结失败模式均主要为黏附性。
本研究表明,使用 Mtwo 锉单独或联合使用 Endosolv R 进行根管再治疗后,Resilon/Epiphany SE 的黏结强度与未处理标本无显著差异。氯仿用于再治疗会对根管再填充后 Resilon/Epiphany SE 的黏结强度产生不利影响。