Division of Oral Health Sciences, Hiroshima University Graduate School of Biomedical Sciences, Minami-ku, Hiroshima, Japan.
Dent Mater J. 2010 Jan;29(1):25-9. doi: 10.4012/dmj.2009-039.
The purpose of this study was to evaluate the effect of primers on bonding between a silver-palladium-copper-gold alloy and an indirect composite material. Cast disks were air-abraded with alumina, conditioned with one of five primers (Alloy Primer, Luna-Wing Primer, Metal Primer II, Metaltite, M.L. Primer), and bonded with a light-activated indirect composite. Shear bond strengths were determined after 20,000 times of thermocycling. The results showed that four of the primers, except the Luna-Wing Primer, were effective in enhancing the bond strength as compared with the unprimed control group. Of these four primers, Alloy Primer, Metal Primer II, and M.L. Primer exhibited significantly greater bond strengths. It can be concluded that the effectiveness of primers varies considerably according to the organic sulfur compounds added to the solvent, and that care must be taken in selecting priming agents for bonding the composite material and the silver-palladium-copper-gold alloy.
本研究旨在评估底涂剂对银钯铜金合金与间接复合树脂之间粘结的影响。铸造盘用氧化铝喷砂处理,用五种底涂剂(Alloy Primer、Luna-Wing Primer、Metal Primer II、Metaltite、M.L. Primer)之一进行预处理,并用光固化间接复合树脂粘结。经过 20000 次冷热循环后测定剪切粘结强度。结果表明,除了 Luna-Wing Primer 以外的四种底涂剂与未处理对照组相比,均能有效提高粘结强度。这四种底涂剂中,Alloy Primer、Metal Primer II 和 M.L. Primer 的粘结强度显著更高。由此可见,底涂剂的有效性根据添加到溶剂中的有机硫化合物而有很大差异,在选择用于粘结复合材料和银钯铜金合金的底涂剂时应谨慎。