State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, Wuhan University of Technology, Wuhan, 430070, P. R. China.
Dalton Trans. 2010 Jul 7;39(25):5860-7. doi: 10.1039/c0dt00053a. Epub 2010 May 27.
Mesporous anatase-phase TiO(2) hollow spheres with high photocatalytic activity were prepared by hydrothermal treatment and self-transformation of amorphous TiO(2) solid spheres in an NH(4)F aqueous solution. The prepared samples were characterized by X-ray diffraction, scanning and transmission electron microscopy, X-ray photoelectron spectroscopy, N(2) adsorption-desorption isotherms and UV-vis absorption spectroscopy. The photocatalytic activity was evaluated by photocatalytic oxidation decomposition of acetone in air under UV irradiation. It is found that F(-) plays an essential role in the formation of TiO(2) hollow spheres. F(-) not only induces the hollowing of TiO(2) solid spheres, but also promotes the crystallization of anatase TiO(2) nanocrystals. A possible formation mechanism for the TiO(2) hollow spheres by localized Ostwald ripening or chemically induced self-transformation is proposed based on the experimental observations. Furthermore, the molar ratios of NH(4)F to TiO(2) (R) exhibit a significant influence on the morphology and photocatalytic activity of the TiO(2) samples. The photocatalytic activity of the samples prepared in the presence of NH(4)F is higher than that of TiO(2) sample prepared in pure water and commercial Degussa P25 (P25) powders. Especially, the TiO(2) hollow spheres prepared at R = 1 show the highest photocatalytic activity and the specific rate constant S(k) exceeds that of P25 by a factor of more than two.
具有高光催化活性的介孔锐钛矿相 TiO(2) 空心球是通过在 NH(4)F 水溶液中热处理和无定形 TiO(2) 固体球的自转化制备的。所制备的样品通过 X 射线衍射、扫描和透射电子显微镜、X 射线光电子能谱、N(2)吸附-解吸等温线和紫外-可见吸收光谱进行了表征。通过在紫外光照射下空气中的丙酮光催化氧化分解评价了光催化活性。研究发现,F(-) 在 TiO(2)空心球的形成中起着至关重要的作用。F(-)不仅诱导 TiO(2) 固体球的空心化,而且促进锐钛矿 TiO(2) 纳米晶的结晶。基于实验观察,提出了一种通过局部奥斯特瓦尔德熟化或化学诱导自转化形成 TiO(2)空心球的可能形成机制。此外,NH(4)F 与 TiO(2)(R)的摩尔比对 TiO(2)样品的形态和光催化活性有显著影响。在存在 NH(4)F 的情况下制备的样品的光催化活性高于在纯水中和商业 Degussa P25(P25)粉末中制备的 TiO(2)样品。特别是,在 R = 1 时制备的 TiO(2)空心球表现出最高的光催化活性,比 P25 的比速率常数 S(k)高两倍以上。