Department of Prosthodontics, Faculty of Dentistry, University of Cumhuriyet, 58140, Sivas, Turkey.
Lasers Med Sci. 2011 Nov;26(6):783-8. doi: 10.1007/s10103-010-0825-6. Epub 2010 Aug 21.
Failure of the bond between the acrylic resin and resilient liner material is commonly encountered in clinical practice. The purpose of this study was to investigate the effect of different surface treatments (sandblasting, Er:YAG, Nd:YAG, and KTP lasers) on tensile bond strength of silicone-based soft denture liner. Polymethyl methacrylate test specimens were fabricated and each received one of eight surface treatments: untreated (control), sandblasted, Er:YAG laser irradiated, sandblasted + Er:YAG laser irradiated, Nd:YAG laser irradiated, sandblasted + Nd:YAG laser irradiated, KTP laser irradiated, and sandblasted + KTP laser irradiated. The resilient liner specimens (n = 15) were processed between two polymethyl methacrylate (PMMA) blocks. Bonding strength of the liners to PMMA were compared by tensile test with the use of a universal testing machine at a crosshead speed of 5 mm/min. Kruskal-Wallis and Wilcoxon tests were used to analyze the data (α = 0.05). Altering the polymethyl methacrylate surface by Er:YAG laser significantly increased the bond strengths in polymethyl methacrylate/silicone specimens, however, sandblasting before applying a lining material had a weakening effect on the bond. In addition, Nd:YAG and KTP lasers were found to be ineffective for increasing the strength of the bond.
在临床实践中,经常会遇到丙烯酸树脂和弹性衬里材料之间的粘结失败。本研究的目的是研究不同表面处理(喷砂、Er:YAG、Nd:YAG 和 KTP 激光)对硅橡胶软衬材料拉伸粘结强度的影响。制作了聚甲基丙烯酸甲酯测试样本,并对其进行了八种表面处理中的一种处理:未处理(对照)、喷砂、Er:YAG 激光照射、喷砂+Er:YAG 激光照射、Nd:YAG 激光照射、喷砂+Nd:YAG 激光照射、KTP 激光照射和喷砂+KTP 激光照射。弹性衬里样本(n = 15)在两块聚甲基丙烯酸甲酯(PMMA)块之间加工。使用万能试验机以 5mm/min 的十字头速度进行拉伸试验,比较衬里与 PMMA 的粘结强度。使用 Kruskal-Wallis 和 Wilcoxon 检验对数据进行分析(α = 0.05)。改变 Er:YAG 激光的 PMMA 表面显著提高了 PMMA/硅橡胶样本的粘结强度,然而,在施加衬里材料之前喷砂处理会削弱粘结强度。此外,Nd:YAG 和 KTP 激光被发现对增加粘结强度无效。