Brewer J D, Garlapo D A, Chipps E A, Tedesco L A
Department of Fixed Prosthodontics, State University of New York, School of Dental Medicine, Buffalo.
J Prosthet Dent. 1990 Dec;64(6):631-4. doi: 10.1016/0022-3913(90)90284-j.
Precementation refinements of porcelain-fused-to-metal crowns often require reglazing or polishing of the porcelain surface. This study was done to determine whether visual inspection differences exist between glazed and polished porcelain surfaces. Prosthodontists, general dentists, and students (six in each group) rated esthetic properties of 12 porcelain-fused-to-metal crowns. All crowns were initially autoglazed. For phase 1 observations, six crowns were air abraded and polished and six retained their glazed surface. For phase 2 observations, the surface treatments were reversed. At both observations, crowns were rated on 5-point Likert scales for outline form, porosity, smoothness, reflectance, texture, dullness, defects, and general esthetic appearances. Phase 1 polished and glazed crowns had different means for outline form sharpness, porosity, reflectance, dullness, and general esthetic appearance. Phase 2 crowns were different for dullness. Polished and glazed crowns alike were more dull at phase 1 than at phase 2. Glazed crowns were different between phases for reflectance and general esthetic appearance. All reported differences were significant at p less than .01. Significant differences occurred among raters with polished and glazed crowns for several variables.
烤瓷熔附金属全冠的黏结前精细处理通常需要对瓷表面进行再上釉或抛光。本研究旨在确定上釉和抛光后的瓷表面在视觉检查上是否存在差异。修复医师、普通牙医和学生(每组6人)对12个烤瓷熔附金属全冠的美学性能进行评分。所有全冠最初均进行了自动上釉。在第1阶段观察中,6个全冠进行了喷砂和抛光,6个保留其釉面。在第2阶段观察中,表面处理方式颠倒。在两次观察中,根据轮廓形态、孔隙率、光滑度、反射率、质地、色泽、缺陷和总体美学外观等5级李克特量表对全冠进行评分。第1阶段中,抛光和上釉的全冠在轮廓形态清晰度、孔隙率、反射率、色泽和总体美学外观方面均值不同。第2阶段全冠在色泽方面存在差异。抛光和上釉的全冠在第1阶段均比第2阶段更显色泽暗沉。上釉全冠在不同阶段的反射率和总体美学外观方面存在差异。所有报告的差异在p值小于0.01时具有统计学意义。在几个变量方面,不同评分者对抛光和上釉全冠的评价存在显著差异。